Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
9.44 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
9.44 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C | 9.44 µin/in-°F | ASTM D696 |
Kuraray Genestarâ„¢ G1352A-M41 Nylon, 35% Glass Filled Low friction reinforced injection grade.Main Features:Low friction coefficientAbrasion resistanceExamples of applications:Friction and wear applicationGear and wheel |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
9.44 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced Vypet VNT 340 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric StrengthFeatures: High temperature performanc.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 150 °C |
9.44 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM AR9300 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
9.44 µin/in-°F @Temperature -58.0 - 122 °F |
1 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
9.44 µin/in-°F @Temperature -58.0 - 122 °F |
1 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C | 9.44 µin/in-°F | ISO 11359-2 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
9.44 µin/in-°F @Temperature -58.0 - 122 °F |
1 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
9.44 µin/in-°F @Temperature -58.0 - 122 °F |
1 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
9.44 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PF00C is a compound based on PA6 resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
9.44 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DEP32 PC LNP* STAT-KON* DEP32 is a compound based on Polycarbonate containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
9.44 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP PF00CS PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PF00CS is a compound based on PA6 resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
9.44 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXC PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC004SXC is a compound based on PA66 resin containing Carbon Fiber. Added features include: Electrically Conductive, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
9.44 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RC004SXS is a compound based on PA 66 resin containing Carbon Fiber. Added features include; Heat Stabilized, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C | 9.44 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America E 2748A Short Glass Fiber Reinforced Epoxy E 2748A is a glass reinforced epoxy molding compound, with good impact strength combined with soft flow for the encapsulation of devices requiring high quality and thermal shock resistance.Informati.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 150 °C |
9.44 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 228 |
DuPont Performance Polymers VESPEL TP-8311 Polyimide Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in both dry and lubricated high temperature environmentsInformation provided b.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C | 9.44 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C | 9.44 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
9.44 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
9.44 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG8 PA6, 40% Glass Fiber Filled, Injection Molded Staramide BG8 is a 40% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
9.44 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
9.44 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/2 |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
9.44 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
9.44 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
9.44 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret.. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
9.44 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RV00CEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00CE is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 20.0 °C |
9.44 µin/in-°F @Temperature 68.0 °F |
TMA |
Sumitomo Bakelite North America RX® 655 Novolac Phenolic Fiberglass and mineral reinforced phenolic molding compound with very high fill level (75%). Excellent dimensional stability and good strength at elevated temperatures. Very low thermal expansion .. |
|||
CTE, linear, Parallel to Flow | 17.0 µm/m-°C @Temperature 23.0 °C |
9.44 µin/in-°F @Temperature 73.4 °F |
TMA |
Sumitomo Bakelite North America RX® 865M Fiberglass Reinforced Phenolic Novolac RX 865M is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |