Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Transformation Temperature = 100 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature 95.0 - 100 °C
203 - 212 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 551 DU 20 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 95.0 - 100 °C
203 - 212 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 551 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 95.0 - 100 °C
203 - 212 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 551 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 95.0 - 100 °C
203 - 212 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 551 WU 20 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 95.0 - 100 °C
203 - 212 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 551 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 95.0 - 100 °C
203 - 212 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 551 WU 80 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Copyright © lookpolymers.com All Rights Reserved