Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 104 °C | 219 °F | Internal method |
Polimeri Europa Riblene® MV 10 Low Density Polyethylene - Injection Molding Riblene MV 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 are highly flexible.Main Applications: Riblene MV 10 is ideal for injection moldi.. |
|||
Melting Point | 104 °C | 219 °F | Internal method |
Polimeri Europa Riblene® MV 10 R Low Density Polyethylene - Injection Molding Riblene MV 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 R are highly flexible.Main Applications: Riblene MV 10 R is ideal for injection.. |
|||
Melting Point | 104 °C | 219 °F | Internal Method |
Polimeri Europa Greenflex® FD 20 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 20 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Films produced with Greenflex FD 20 exhibit good optical properties, high impact resistance, tensile .. |
|||
Melting Point | 104 °C | 220 °F | |
M. Holland Company MAGMA® LM112-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melting Point | 104 °C | 219 °F | Exxon Method |
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Melting Point | 104 °C | 219 °F | Exxon Method |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Melting Point | 104 °C | 219 °F | Exxon Method |
ExxonMobil Escorene® LD-317 EVA Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 5.5% vinyl acetate copolymer film resin. Film made from LD-317 offers excellent impact strength, tensile properties, and h.. |
|||
Melting Point | 104 °C | 219 °F | ASTM D3418 |
LyondellBasell Microthene® G MN71020 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melting Point | 104 °C | 219 °F | ASTM D3418 |
LyondellBasell Microthene® G MN71120 Low Density Polyethylene (Rotomolding) General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melting Point | 104 °C | 219 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5021 400 Micron LDPE Powder Description: ICOFLO 510-5021 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 104 °C | 219 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5059 500 Micron LDPE Powder Description: ICOFLO 510-5059 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 104 °C | 219 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5060 800 Micron LDPE Powder Description: ICOFLO 510-5060 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a barrier in ma.. |
|||
Melting Point | 104 °C | 219 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5061 1200 Micron LDPE Powder Description: ICOFLO 510-5061 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 104 °C | 219 °F | DSC; ASTM D3418 |
ICO Polymers ICOTEXâ„¢ 520-5059 500 Micron LDPE Powder Description: ICOTEX 520-5059 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Information provided by ICO Polymers.A Sch.. |
|||
Melting Point | 104 - 113 °C | 219 - 235 °F | |
Indium Corp. Indalloy 56 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 104 °C | 219 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating 6.5 wt% Methacrylic Acid.Nucrel® 0609HSA is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment.. |
|||
Melting Point | 104 °C | 219 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res.. |
|||
Melting Point | 104 °C | 219 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 200.48 Extrusion Coating and Laminating Resin Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala.. |
|||
Melting Point | 104 °C | 219 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 202.48 Extrusion Coating Resin Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro.. |
|||
Melting Point | 104 °C | 220 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 334.82 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1003 VL 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the .. |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1005 VN 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process.Applications Grade for transparent and resistant film production. Examples: curtain stretch, coextrusion, stretch hood.ISO data provided by the ma.. |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1005 VG 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for strength films, sealable at low temperature with some hot tack. Examples: rigid bags, deep-freeze packaging, laminates, co.. |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1020 VG 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for resistant films, sealable at low temperature with some hot tack. Examples: bags, deep-freeze packaging, laminates, coextru.. |
|||
Melting Point | 104 - 113 °C | 219 - 235 °F | Average value: 108 °C Grade Count:11 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Melting Point | 104 - 127 °C | 220 - 261 °F | Average value: 125 °C Grade Count:28 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |
|||
Melting Point | 104 °C | 219 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 0609HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinue 6 wt% Methacrylic Acid.Nucrel® 0609HS* (High-Speed) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminatin.. |