Polymer Property : Melting Point = 128 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 88.0 - 128 °C
190 - 262 °F
Hybrid Plastics POSS® MA0717 MethacrylEthyl-POSS®
POSS® Nanostructured Chemical Technology has two unique features: (1) the chemical composition is a hybrid, intermediate (RSiO1.5) between that of silica (SiO2) and silicones (R2SiO). (2) POSS®..
Melting Point 118 - 128 °C
244 - 262 °F
MQSA 111
Lubrizol Advanced Materials PEARLCOAT® DIPP-119 Thermoplastic Polyurethane Elastomer
PEARLCOAT® DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this product..
Melting Point 125.6 - 128 °C
258.1 - 262 °F
Solvay Chemicals Ammonium Hydrogen Fluoride
Ammonium hydrogenfluoride (NH4HF2) is used for aluminum anodization, metal surface treatment, manufacture of wood preservatives, glass processing, building protection, mineral oil/ natural gas drill..
Melting Point 75.0 - 128 °C
167 - 262 °F
Average value: 113 °C Grade Count:36
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..
Melting Point 126 - 128 °C
259 - 262 °F
Average value: 126 °C Grade Count:5
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max..
Melting Point 124 - 128 °C
255 - 262 °F
Average value: 127 °C Grade Count:5
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and..
Melting Point 125 - 128 °C
257 - 262 °F
Average value: 126 °C Grade Count:11
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i..