Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 1000 PE-UHMW, Black OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | DSC ISO 3146 |
Okulen® 1000 PE-UHMW, Green Black OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 135 °C | 275 °F | Internal method |
Polimeri Europa Eraclene® ML 70 U High Density Polyethylene - Injection Molding Eraclene ML 70 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution. It combin.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data) TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet) |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® ESD Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) Protects against electrical charge build-up Reduces noise Self-lubricating Corrosion-resistant No moisture absorption |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® MD UHMW-PE, FDA Metal Detectable (ASTM Product Data Sheet) Meets FDA and USDA guidelines; 3-A Dairy-approved (natural) Reduces noise Self-lubricating Chemical-, corrosion- and wear-resistant No moisture absorption Non-toxic, low-friction surface Meets ASTM.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, OF OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 182 °C | 275 - 360 °F | Average value: 157 °C Grade Count:26 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Melting Point | 135 - 254 °C | 275 - 489 °F | Average value: 237 °C Grade Count:17 |
Overview of materials for Nylon 66 Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66 Fiber". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Melting Point | 135 °C | 275 °F | |
LyondellBasell Lupolen® 6021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small, rigid, thin-walled containers (up to 5 l), pots (up to 1 l), bottles and canisters (up to 5 l) for packaging mineral oil, antifreeze, brake fluid; drink bott.. |
|||
Melting Point | 135 °C | 275 °F | 10°C/min; ASTM D3418 |
LG Chemical SEETEC PF150 HDPE Features: Characteristics: Good impact & tear strength, High speed & superior heat sealing propertiesAdditives: Anti-oxidants, LubricantsApplication: Shopping bags, Thin films, Trash bags, Multiwall.. |
|||
Melting Point | 135 °C | 275 °F | MTM 15902 |
LyondellBasell Adsylâ„¢ 5 C 30 F Polyolefin Description: Adsylâ„¢ 5 C 30 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity a.. |
|||
Melting Point | 135 °C | 275 °F | |
Heatbath/Park Low Temperature Draw Salt Quenching and Tempering Salt A eutectic mixture offering the lowest melting point and a wide working range. Formulated per MIL-S-10699-B, Class 1 (275 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical... |
|||
Melting Point | 135 - 145 °C | 275 - 293 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp.. |
|||
Melting Point | 135 °C | 275 °F | |
Techmer ES HiFill® HDPE TM10 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 135 °C | 275 °F | |
Techmer ES HiFill® HDPE TM20 UV BK 20% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: BlackInformation provided by TP Composi.. |
|||
Melting Point | 135 °C | 275 °F | |
Techmer ES HiFill® HDPE TM25 25% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 25% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 135 °C | 275 °F | Kofler |
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good low temperature properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and .. |
|||
Melting Point | 135 - 145 °C | 275 - 293 °F | Sheath |
EMS-Griltech Grilon® BA 140 White Nylon 66/CoPA Bi-Component Fiber Description: GRILON BA 140 is the new core / sheath bi-component fiber based on PA 6/CoPA with a sheath melting range from 135 - 145 °C. The fine count bi-component fiber guarantees an even distrib.. |
|||
Melting Point | 135 °C | 275 °F | (Dry) |
Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema. |
|||
Melting Point | 135 °C | 275 °F | 10°C/min |
Arkema Group Kynar® FLEX 2750 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1NS, M. ?E7.B.F.A.C,, ? (4-10)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousne.. |
|||
Melting Point | 135 °C | 275 °F | Internal method |
Polimeri Europa Eraclene® MM 84 U High Density Polyethylene - Injection Molding Eraclene MM 84 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 U is characterized by high rigidity and good impac.. |
|||
Melting Point | 135 °C | 275 °F | DSC |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |