Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 1595 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1595 - 1675 °C
2903 - 3047 °F
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + Annealed
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. ..
Melting Point 1595 - 1675 °C
2903 - 3047 °F
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®..
Melting Point 1595 - 1675 °C
2903 - 3047 °F
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 20% Elongated Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 20% Elongated Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL..
Melting Point 1595 - 1675 °C
2903 - 3047 °F
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Elongated Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Elongated Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL..
Melting Point 1595 - 1675 °C
2903 - 3047 °F
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + Annealed
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. ..
Melting Point 1595 - 1675 °C
2903 - 3047 °F
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®..
Melting Point 1595 - 1675 °C
2903 - 3047 °F
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STOA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STOA (885°C/1hr/AC + 705°C/1hr/AC) condition. Other data below are typical of TIMETAL..
Melting Point 1595 - 1675 °C
2903 - 3047 °F
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Typical
This entry has typical property data. Other database entries for TIMETAL® 6-2-4-6 have tensile and fatigue data for specific sample conditions.High-Strength, Intermediate Temperature AlloyFeatures..
Melting Point 1595 - 1675 °C
2903 - 3047 °F
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Beta Forged + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the Beta Forged + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4..
Copyright © lookpolymers.com All Rights Reserved