Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 103 °C | 217 °F | Internal Method |
Polimeri Europa Greenflex® FL 25 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FL 25 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FL 25 show good optical properties and excellent sealability.Main Applications: .. |
|||
Melting Point | 103 °C | 217 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 103 - 110 °C | 217 - 230 °F | |
Pau Tai Cadmium stearate, Monomer Stabilizer Transparent heat resistance stabilizer. Excellent effect if used with barium and tin series stabilizer. Excellent lubricant at high temperature operation.Applications: Rigid processing, adhesive pla.. |
|||
Melting Point | 103 °C | 217 °F | Exxon Method |
ExxonMobil Escorene® LD-306 EVA Film Resin, High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.5% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |
|||
Melting Point | 103 °C | 217 °F | Exxon Method |
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze.. |
|||
Melting Point | 103 °C | 217 °F | Exxon Method |
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne.. |
|||
Melting Point | 103 °C | 217 °F | Exxon Method |
ExxonMobil Escorene® LD-334 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.2% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Melting Point | 103 - 105.3 °C | 217 - 221.5 °F | |
Hong Kun Group UV 329 UV Absorber A highly effective light stabilizer, it has a broad UV absorption spectrum and low volatility. For PS, polymethyl methacrylate, unsaturated polyester (UPE), rigid PVC, polycarbonate, ABS resin, etc... |
|||
Melting Point | 103 - 105 °C | 217 - 221 °F | |
M Chemical GUARD DOGâ„¢ UV5411 Benzotriazole UV Absorber, Powder and LD Pellet GUARD DOGâ„¢ UV5411 light stabilizer is a derivative of Benzotriazole that has exceptionally strong and broad-range UV absorption properties throughout the UV spectrum. It is highly recommended .. |
|||
Melting Point | 103 - 227 °C | 217 - 441 °F | |
Indium Corp. Indalloy 217-440 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 103 °C | 217 °F | 10°C/min; ASTM D3418 |
LG Chemical SEETEC EF221 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical Properties Additives: Antiblocking agent, Slip AgentApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical |
|||
Melting Point | 103 - 113 °C | 217 - 235 °F | |
Fine Organics FINALUX GT 25 Composite Lubricant Applications: One pack lubricant specially suggested for RPVC pressure pipes and commercial pipes, suitable for single as well as twin screw extruders.Information provided by Fine Organics |
|||
Melting Point | 103 - 117 °C | 217 - 243 °F | |
Indium Corp. Indalloy 58 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 103 °C | 217 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 41E687 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Melting Point | 103 °C | 217 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating 9.2 wt% Methacrylic Acid.Nucrel® 0908HS is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and blown/cast film operations desi.. |
|||
Melting Point | 103 °C | 217 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 0910HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating 8.7 wt% Methacrylic Acid.Nucrel® 0910HS (High-Stability) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating and extrusion lamin.. |
|||
Melting Point | 103 °C | 217 °F | Peak DSC; Westlake Method |
Westlake Elevate™ EF563 6.5% Ethylene Vinyl Acetate Copolymer Westlake EF 563 resin is a fractional melt index 6.5% EVA copolymer with excellent drawdown, low melting/dispersion, and clarity optics in a soft but very tough film. Kosher compliant.Application/U.. |
|||
Melting Point | 103 °C | 217 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Melting Point | 103 °C | 217 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 41E850 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Melting Point | 103 °C | 217 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 307.76 Clear, High Impact Film Resin LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical |
|||
Melting Point | 103 °C | 217 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD331.08 EVA LD 331.08 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |
|||
Melting Point | 103 °C | 217 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD331.99 EVA LD 331.99 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |
|||
Melting Point | 103 °C | 217 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8445 Polyolefin Elastomer Description: Engage® 8445 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p.. |
|||
Melting Point | 103 - 107 °C | 217 - 225 °F | |
C.O.I.M. FILCO® 657 Unsaturated Polyester Powder Resin Description: Unsaturated Polyester Powder ResinGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and a.. |
|||
Melting Point | 103 °C | 217 °F | |
M. Holland Company MAGMA® LM213-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melting Point | 103 °C | 217 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8540 Polyolefin Elastomer Description: Engage® 8540 polyolefin elastomer is an ethyleneoctene copolymer that is well suited to foamed applications and offers excellent performance for profile extrusion of tubing and hoses. .. |
|||
Melting Point | 103 °C | 217 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 0910HS-SR Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating
(discontinued **)< 8.7 wt% Methacrylic Acid.Nucrel® 0910HS-SR is an ethylene-methacrylic acid copolymer resin available for use in conventional and coextrusion coating equipment designed to process polyethylene resin.. |