Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 104 °C | 219 °F | Internal method |
Polimeri Europa Riblene® MV 10 Low Density Polyethylene - Injection Molding Riblene MV 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 are highly flexible.Main Applications: Riblene MV 10 is ideal for injection moldi.. |
|||
Melting Point | 104 °C | 219 °F | Internal Method |
Polimeri Europa Greenflex® FD 23 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 23 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Greenflex FD 23 is a version of Greenflex FD 20 with added slip and antiblocking agents. Films produ.. |
|||
Melting Point | 104 °C | 219 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 509.48 Compounding Resin
(discontinued **) LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications.Information provided by ExxonMobil Chemical |
|||
Melting Point | 104 °C | 219 °F | Exxon Method |
ExxonMobil Escorene® LD-402 LDPE Electrical Jacketing Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low density polyethylene homopolymer resin designed for high speed extrusions. |
|||
Melting Point | 104 °C | 219 °F | Exxon Method |
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Melting Point | 104 °C | 219 °F | Exxon Method |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Melting Point | 104 °C | 219 °F | Exxon Method |
ExxonMobil Escorene® LD-317 EVA Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 5.5% vinyl acetate copolymer film resin. Film made from LD-317 offers excellent impact strength, tensile properties, and h.. |
|||
Melting Point | 104 °C | 219 °F | ASTM D3418 |
LyondellBasell Microthene® G MN71020 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melting Point | 104 °C | 219 °F | ASTM D3418 |
LyondellBasell Microthene® G MN71120 Low Density Polyethylene (Rotomolding) General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melting Point | 104 °C | 219 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5059 500 Micron LDPE Powder Description: ICOFLO 510-5059 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 104 °C | 219 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5060 800 Micron LDPE Powder Description: ICOFLO 510-5060 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a barrier in ma.. |
|||
Melting Point | 104 °C | 219 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating 6.5 wt% Methacrylic Acid.Nucrel® 0609HSA is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment.. |
|||
Melting Point | 104 °C | 219 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res.. |
|||
Melting Point | 104 °C | 219 °F | ISO 11357 |
Total EVA 1005 VN 2 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 2 is made by a high pressure tubular process. Grade for transparent and resistant films. Contains an antioxidant.Application examples: Stretch, coextrusion, frozen food, agriculture fi.. |
|||
Melting Point | 104 °C | 219 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 202.48 Extrusion Coating Resin Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro.. |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1003 VL 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the .. |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1005 VN 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process.Applications Grade for transparent and resistant film production. Examples: curtain stretch, coextrusion, stretch hood.ISO data provided by the ma.. |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1020 VB 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for transparent, resistant films, sealable at low temperature. Examples: laminates.ISO data provided by the manufacturer, Arke.. |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1020 VB 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding rigid articles. Examples: closures, ice trays.ISO data provided by the manufacturer, Arkema. |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1005 VG 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for strength films, sealable at low temperature with some hot tack. Examples: rigid bags, deep-freeze packaging, laminates, co.. |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1005 VL 2C Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Grade for thermal agricultural films to 180 at 200 µ with diffusing effect, for greenhouse coverage.ISO d.. |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1006 VL 2E Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 200 at 210 µm for greenhouse coverage.ISO data provided by the.. |
|||
Melting Point | 104 °C | 219 °F | 10°C/min |
Arkema Group Evatane® 1020 VG 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for resistant films, sealable at low temperature with some hot tack. Examples: bags, deep-freeze packaging, laminates, coextru.. |
|||
Melting Point | 104 - 113 °C | 219 - 235 °F | Average value: 108 °C Grade Count:11 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Melting Point | 104 - 200 °C | 219 - 392 °F | Average value: 113 °C Grade Count:15 |
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an.. |
|||
Melting Point | 104 °C | 219 °F | Freezing Point; ASTM D3418 |
DuPont Surlyn® PC2000