Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 105 °C | 221 °F | Exxon Method |
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi.. |
|||
Melting Point | <= 105 °C | <= 221 °F | |
Kazanorgsintez NMPE-1 Low-Molecular Polyethylene Low-molecular polyethylene of high pressure polyethylene production. Application: Designed for use in the rubber industry, building industry, and other fields. Can also be used as component parts.. |
|||
Melting Point | 105 - 115 °C | 221 - 239 °F | |
Fine Organics FINAWAX KD Lubricant Additive Applications: Non-oxidised polyethylene wax for rigid PVC extrusion.Information provided by Fine Organics |
|||
Melting Point | 105 °C | 221 °F | 10°C/min; ASTM D3418 |
LG Chemical SEETEC BC500 LDPE Good Processability and Good electrical properties. Main Application: Cable insulationCAS No. 9002-88-4Information provided by LG Chemical |
|||
Melting Point | 105 °C | 221 °F | 10°C/min; ASTM D3418 |
LG Chemical SEETEC BS500 LDPE Characteristics: Good Processability and Good cell uniformity& stability Additives: Antioxidant, Antiblocking agent, Slip AgentApplications: Foam sheetInformation provided by LG Chemical |
|||
Melting Point | 105 °C | 221 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ LD1630J Low Density Polyethylene Injection Molding Key Characteristics:Good flowability for multicavitiesGood toughness and flexibilityExcellent gloss and transparencyOdorlessSafe for food contactRecommended Applications:HousewaresSmall to large clo.. |
|||
Melting Point | 105 °C | 221 °F | 10°C per minute; ISO 3146 |
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap.. |
|||
Melting Point | 105 °C | 221 °F | 10°C per minute; ISO 3146 |
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap.. |
|||
Melting Point | 105 °C | 221 °F | DSC; ASTM D3418 |
DuPont Appeel® LSR11D542 Lidding Sealant Resin Appeel® LSR11D542 is a modified ethylene vinyl acetate copolymer resin designed to function as a peelable sealing layer for lidding and pouch applications. It provides a peelable seal and a "whiten.. |
|||
Melting Point | 105 °C | 221 °F | DSC; ASTM D3418 |
DuPont Bynel® 42E703 Adhesive Resin Bynel® Series 4200 resins are anhydride-modified low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 105 °C | 221 °F | 10°C per minute; ISO 3146 |
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap.. |
|||
Melting Point | 105 °C | 221 °F | 10°C per minute; ISO 3146 |
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap.. |
|||
Melting Point | 105 °C | 221 °F | 10°C per minute; ISO 3146 |
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap.. |
|||
Melting Point | 105 - 115 °C | 221 - 239 °F | DSC |
EMS-Griltech Griltex® 11A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 105 - 115 °C | 221 - 239 °F | DSC |
EMS-Griltech Griltex® D 1299A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 105 - 115 °C | 221 - 239 °F | DSC |
EMS-Griltech Griltex® D 1564A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications) GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent r.. |
|||
Melting Point | 105 °C | 221 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 302.34 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Melting Point | 105 °C | 221 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 302.56 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Melting Point | 105 °C | 221 °F | Dow Method (DSC) |
Dow 722 Low Density Polyethylene (LDPE) Polyethylene 722 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry foods packaging, snack foods packaging, moist foods pac.. |
|||
Melting Point | 105 °C | 221 °F | DSC |
Arkema Group LOTADER® 4210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 4210 is a versatile adhesive for extrusion coating or lam.. |
|||
Melting Point | 105 °C | 221 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 206.48 Extrusion Coating Resin
(discontinued **) LD 206.48 is a extrusion coating grade, having good organoleptic properties compared to existing standard low odor/off-taste LDPE extrusion coating polymers.Information provided by ExxonMobil Chemic.. |