Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 223 - 225 °C | 433 - 437 °F | |
Plastcom SLOVASTER® B/A GF 20 PBT, 20% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Melting Point | 223 - 225 °C | 433 - 437 °F | |
Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Melting Point | 200 - 225 °C | 392 - 437 °F | Average value: 223 °C Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Melting Point | 165 - 225 °C | 329 - 437 °F | Average value: 205 °C Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | Average value: 224 °C Grade Count:10 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | Average value: 218 °C Grade Count:73 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Melting Point | 215 - 225 °C | 419 - 437 °F | Average value: 221 °C Grade Count:62 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | Average value: 218 °C Grade Count:6 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Melting Point | 215 - 225 °C | 419 - 437 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® D11H95S Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H95S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out.. |
|||
Melting Point | 215 - 225 °C | 419 - 437 °F | |
UBE 1026B1 Nylon 6 Homopolymer Film Specialties: Nucleated (High viscosity) Processing: T-die, Air blownApplications: General applicationsInformation provided by UBE. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | |
Tisan TISLAMID® 6 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | |
Tisan TISLAMID® 6 30% Glass Bead Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | |
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 215 - 225 °C | 419 - 437 °F | Sheath |
EMS-Griltech Grilon® BA 3100 White Nylon 66/Nylon 6 Bi-Component Fiber Description: GRILON BA 3100 is the new core / sheath bi-component fiber based on PA 66/PA 6 with a sheath melting range from 215 - 225 °C. The fine count bi-component fiber guarantees an even distr.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 412 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 420 Polyester - PBT, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Hiloy® 617 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.55% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Voloy® 430 Glass Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® B 4406 PBT Description: Is a PBT, flame-retardant injection-molding grades, unreinforced for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting compo.. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 432 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | 10 K/min |
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® S 4090 G6 High Speed 30% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 30% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® S 4090 GM13 5/15% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber and 15% mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventila.. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | Average value: 223 °C Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | ISO 11357-3 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | |
BASF Ultradur B 6550 L PBT Ultradur B 6550 L is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |