Thermal Properties Metric English Comments
Melting Point 230 °C
446 °F
Oceanchem Group 2,4,6-Tris (2,4,6-tribromophenoxy)-1,3,5-triazine (FR245
Molecular Formula: C21H6Br9N3O3Cas No.: 25713-60-4Use: FR245 a brominated cyanurate is a proprietary, additive flame retardant. The comination of aromatic bromine and cyanurate provides high FR eff..
Melting Point 230 °C
446 °F
ISO 11357-3
Pasargad Polymer Peyvand Pasalac 3P-H9000B ABS/PC
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly..
Melting Point 230 °C
446 °F
ISO 11357-3
Pasargad Polymer Peyvand Pasalac 3P-H9000W ABS/PC
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly..
Melting Point >= 230 °C
>= 446 °F
Pau Tai Barium stearate, Monomer Stabilizer
Excellent effect if used with cadmium, zinc, lead. Excellent lubricity and electrical insulation. Resistance to sulfide staining.Applications: Applicable to hard, soft common adhesive plaster, rubbe..
Melting Point 230 °C
446 °F
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)  (Unverified Data**)
Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into..
Melting Point 230 - 246 °C
446 - 475 °F
Limits; M2E-73-002
Indorama Ventures Mexico Polyclearâ„¢ Preserve 2201 PET Resin
Description: La resina Polyclear® Preserve PET 2201 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g y esta disenada para ofrecer un redimiento supe..
Melting Point 230 - 250 °C
446 - 482 °F
Johnson Matthey JM 97C Soft Solder/Flux
General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi..
Melting Point 230 - 235 °C
446 - 455 °F
Johnson Matthey JM 99C Soft Solder/Flux
General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi..
Melting Point 230 °C
446 °F
DSC
Solvay Specialty Polymers Ixef® BXT 2000-0203 Polyarylamide (PARA)
Ixef® BXT 2000-0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef® BXT 2000-0203 resin can be successfully extru..
Melting Point 230 °C
446 °F
Solvay RHODAQUAT® M-242B/99 Surfactant
Description: Rhodaquat® M-242B/99 is high purity cationic surfactant A free flowing crystalline powder has unique property of static and tangling elimination, imparting soft and elegant feel to h..
Melting Point 230 °C
446 °F
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
Melting Point 230 °C
446 °F
Tisan TISARBON® Flame Retardant (V0) Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
Melting Point 230 °C
446 °F
Tisan TISARBON® UNR Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
Melting Point 230 - 282 °C
446 - 540 °F
Zeus ETFE Tubing
ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 051.LQ Low Density Polyethylene Resin
Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding proc..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 100.BW Low Density Polyethylene Resin
Product Description: LD 100.BW is a LDPE grade, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.Ava..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 100AC Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 100BR Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin (European Grade)
Product Description: LD 100BW is a LDPE containing low antioxidants suitable for the production of LV and MV crosslinked insulation using the 1-step or 2-step silane technology. Through in-house com..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 101BA Wire & Cable Low Density Polyethylene Resin
Product Description: LD 101BA Wire & Cable is anon-stabilized LDPE, designed for the production of Medium/High Voltage insulation using the direct peroxide addition. For cleanliness reasons, the mat..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 185BW Low Density Polyethylene Resin (European Grade)
Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 185GE Low Density Polyethylene Resin (European Grade)
Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 185JD Low Density Polyethylene Resin (European Grade)
Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 503.LP Low Density Polyethylene Resin
Product Description: LD 503.LP is a LDPE homopolymer that is suitable for use in molding, extrusion, compounding and foam applications.Availability: Latin America, North America and South AmericaAdd..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 506.07 Low Density Polyethylene Resin
Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 516.LN Low Density Polyethylene Resin
Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un..
Melting Point <= 230 °C
<= 446 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin
Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is..
Melting Point 230 °C
446 °F
HG/T2235
Beijing Evergrow Resources MoS2 Filled Nylon
Information provided by Beijing Evergrow Resources.
Copyright © lookpolymers.com All Rights Reserved