Polymer Property : Melting Point = 280 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 138 °C
280 °F
Multibase Multi-Flex® TPE D 4502 BLK
Multi-Flex® D 4502 is based on Shell's Kraton G polymer and is suitable for applications for the automotive industry. It exhibits excellent paintability adhesion and is recommended as substrate fo..
Melting Point 138 °C
280 °F
Multibase Multi-Flex® TPO D 4508 D 4508
This product is suitable for airbag enclosures and is based on polyolefins/kraton rubber, exhibiting good paintability and low temperature performance.Data provided by Multibase.
Melting Point 138 °C
280 °F
Flow temperature, ASTM D569-59
Rotuba 860MS 686.5 Ethyl Cellulose
Data provided by the manufacturer.
Melting Point 138 °C
280 °F
Internal method
Polimeri Europa Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin
Eraclene PF 92 is a homopolymer high density polyethylene resin (HDPE) with antioxidants, suitable for pipe application. It is characterized by high rigidity, high impact strength and low swelling...
Melting Point 138 °C
280 °F
Flow temperature, ASTM D569
Rotuba MSS Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Melting Point 138 - 148 °C
280 - 298 °F
MQSA 111
Lubrizol Advanced Materials PEARLTHANE® 12K85LB Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mech..
Melting Point 138 °C
280 °F
Flow temperature; ASTM D569
Plaskolite Optix® PL-150 Acrylic Resin  (discontinued **)
Injection/extrusion pellets.Data provided by the manufacturer, Plaskolite, Inc.
Melting Point 138 °C
280 °F
Hong Kun Group UV 326 UV Absorber
UV-326 is a important ultraviolet absorber of bonzotriazoleseries, which is stable, nontoxic, higher absorbency for ultraviolet ray. Widely used for photosensitive materials and poly merized materia..
Melting Point 138 °C
280 °F
Hyosung Topilene C600MU PP
C600MU Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation
Melting Point 138 °C
280 °F
Eutectic
Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy
Good low melting point solder for electronics assembly of for applications where Cd and Pb are to be avoided, and for thermo-electric applications. Shear rate sensitive.Information provided by the m..
Melting Point 138 - 148 °C
280 - 298 °F
Fine Organics FINAWAX C Lubricant Additive
Applications: Antiblock agent for soft PVC films/sheets, strong release agent for rigid PVC calendered sheets, dispersant for FRLS PVC compounds.Information provided by Fine Organics
Melting Point 138 - 170 °C
280 - 338 °F
Indium Corp. Indalloy 281-338 Bismuth-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 138 - 150 °C
280 - 302 °F
Struktol TR EBS Processing Additive, Dispersant
N,N` Ethylene Bis-stearamideSTRUKTOL® TR EBS is an exceptionally effective dispersion aid for a wide range of organic and inorganic pigments. STRUKTOL® TR EBS can be used in most polymer carri..
Melting Point 138 - 144 °C
280 - 291 °F
ISO 3146
Borealis Borclear™ RD738CF Propylene Alpha Olefin Copolymer for Cast Film
Borclear RD738CF is a slip and antiblock formulation propylene alpha olefin copolymer resin. It is suitable for the manufacturing of unoriented film on chill roll process.Borclear RD738CF is suitabl..
Melting Point 138 - 144 °C
280 - 291 °F
ISO 3146
Borealis Borclear™ RE718CF Propylene Alpha Olefin Copolymer for Metallizable Cast Film
Borclear RE718CF is a propylene alpha olefin copolymer resin formulation with antiblocking agent and without Ca-stearate, especially developed for the manufacturing of unoriented cast films for meta..
Melting Point 138 - 142 °C
280 - 288 °F
ISO 3146
Borealis Borsoft™ SD233CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Borsoft SD233CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal..
Melting Point 138 - 142 °C
280 - 288 °F
DSC; ISO 3146
Borealis BorPURE™ RD208CF Polypropylene Random Copolymer
BorPure™ RD208CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. This grade is suitable for the manufacturing of unoriented films o..
Melting Point 138 - 142 °C
280 - 288 °F
ISO 3146
Borealis Borsoft™ SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film
Borsoft SA233CF is a very soft random heterophasic copolymer, suitable for use on conventional blown film lines with air-coolingBorsoft SA233CF is especially suitable for soft packaging, hygienic fi..
Melting Point 138 - 154 °C
280 - 310 °F
DayGlo ZQ Pigments ZQ-18 Signal Green
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Melting Point 138 - 154 °C
280 - 310 °F
DayGlo ZQ Pigments ZQ-19 Horizon Blue
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Melting Point 138 - 170 °C
280 - 338 °F
AIM 40Bi/60Sn Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Melting Point 138 - 170 °C
280 - 338 °F
AIM 54Sn/26Pb/20In Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Melting Point 138 °C
280 °F
AIM 58Bi/42Sn Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Melting Point >= 138 °C
>= 280 °F
Oceanchem Group Hydroxymethylphenylphosphinic Acid (HMPPA)
Molecular Formula: C7H9O3PCas No.: 61451-78-3Application: HMPPA is a bifunctional copolymerisable phosphorous flame retardant monomer, which can be polycondesated with ethylene glycol and terephthal..
Melting Point <= 138 °C
<= 280 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ AD 0633EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: AD 0433EH2 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: ..
Melting Point 138 °C
280 °F
Peak; DSC
ExxonMobil EXXELOR™ PO 1015 Maleic anhydride functionalized polypropylene
Product Description: Exxelor Po 1015 polymer resin is a maleic anhydride fuctionalized polypropylene copolymer, produced by reactive extrusion. It has been primarily designed to add polarity to poly..
Melting Point 138 - 175 °C
280 - 347 °F
Average value: 155 °C Grade Count:9
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..