Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 160 °C | 320 °F | STN EN 11357-1 |
Plastcom PLASTALEN® PH 91 SD Polypropylene Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o. |
|||
Melting Point | 160 °C | 320 °F | |
Plastcom SLOVALEN PH 49 GF 10 GB 20 PP, 20% glass beads, 10% glass fibre, coupling agent FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10 % glass fiber and 20% glass beads, contains themodifier of mechanical properties. Increased strength in comparis.. |
|||
Melting Point | 160 °C | 320 °F | |
Plastcom SLOVALEN PH 59 GF 30 PP, 30% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suita.. |
|||
Melting Point | 160 °C | 320 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Melting Point | 160 °C | 320 °F | |
Plastcom SLOVALEN PH 76 T 20 FRD 5 PP, 20% mineral filling, flame retardant FeaturesModified homopolymer PP for injection moulding, with the content of 20% microground chemically modified talc, retarded with halogen flame retardant Application - electrical industry - termin.. |
|||
Melting Point | 160 °C | 320 °F | |
Plastcom SLOVALEN PH 78 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards detergents. General application in all industry branches.. |
|||
Melting Point | 160 °C | 320 °F | |
Plastcom SLOVALEN PH 99 GB 30 LS PP, 30% glass beads, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Melting Point | 160 - 170 °C | 320 - 338 °F | ASTM D3418 |
NatureWorks® Ingeo™ 3801X Injection Grade PLA Ingeo™ 3801X is designed for injection molding applications that require high heat and high impact performance. This polymer grade has much more rapid crystallization kinetics than other NatureWork.. |
|||
Melting Point | 160 - 170 °C | 320 - 338 °F | Cured State |
Palm Labs Adhesives Turbo Fuse Series 115SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115SI – SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture... |
|||
Melting Point | 160 °C | 320 °F | ISO 11357-3 |
Pasargad Polymer Peyvand Pasalen 3P-H3130B Polypropylene, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Melting Point | 160 °C | 320 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PH 49 GF 10 Polypropylene Homopolymer, 10% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Melting Point | 160 °C | 320 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 160 - 175 °C | 320 - 347 °F | Huntsman/TMA |
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Melting Point | 160 °C | 320 °F | ASTM D2117 |
SCG Chemicals EL-Proâ„¢ P600F Polypropylene Film Resin Key Characteristics:Good optical propertiesHigh productivityGood openability with 3000 ppm slip agent and 2700 ppm antiblocking agentRecommended Applications:Water quenched blown film for food and a.. |
|||
Melting Point | 160 °C | 320 °F | DSC |
Polyram BondyRam® 1001 Maleic Anhydride modified Homo-polypropylene coupling agent Maleic Anhydride modified Homo-polypropylene recommended for coupling of glass and other fillers in polypropylene compositesInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 160 °C | 320 °F | DSC |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | TOTAL Method |
Total PPC 5946WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5946WZ is a nucleated impact copolymer with a Melt Flow index of 75 g/10 min.TOTAL Polypropylene 5946WZ is characterized by very low warpage, improved stiffness, a.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | TOTAL Method |
Total PPC 4720XWZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4720XWZ is a nucleated impact copolymer with a Melt Flow index of 25 g/10 min.TOTAL Polypropylene 4720XWZ is characterized by improved stiffness, creep resistance,.. |
|||
Melting Point | <= 160 °C | <= 320 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 02528CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 02528CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: YesFree .. |
|||
Melting Point | 160 °C | 320 °F | ASTM-D3418 |
CTC X-PRO CTC PP1035 Polypropylene Homopolymer X-PRO PP 1035 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Melting Point | 160 °C | 320 °F | ASTM-D3418 |
CTC X-PRO CTC PP1050 Polypropylene Homopolymer X-PRO PP 1050 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Melting Point | 160 °C | 320 °F | Dow Method (DSC) |
Dow Saran® 2032 Information provided by Dow |
|||
Melting Point | 160 °C | 320 °F | DSC; Dow Method |
Dow H349-02 Polypropylene Homopolymer Resin H349-02 Polypropylene Resin intended for use in biaxial oriented (BOPP) film processes. This product can also be used in extrusion and thermoforming applications where improved melt strength is des.. |
|||
Melting Point | 160 °C | 320 °F | (Dry) |
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema. |
|||
Melting Point | 160 °C | 320 °F | ISO 11357 |
Arkema Group Pebax® 4033 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Melting Point | 160 - 164 °C | 320 - 327 °F | ISO 11357-3 |
Addcomp PRIEX® 20097 Maleic Anhydride Grafted PP homopolymer Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fibre, wood flour, natural fibres, multilayer films, aluminium foils, .. |
|||
Melting Point | 160 °C | 320 °F | |
Plastcom SLOVALEN PH 21 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr.. |
|||
Melting Point | 160 °C | 320 °F | ASTM D789 |
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 160 °C | 320 °F | ASTM D789 |
Adell RZ-14 Copolymer Polypropylene, 20% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 160 °C | 320 °F | ASTM D789 |
Adell RA-16 Copolymer Polypropylene, 30% Talc Filled Data provided by Adell Plastics, Inc. |