Thermal Properties Metric English Comments
Melting Point 155 - 165 °C
311 - 329 °F
MQSA 111
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1..
Melting Point 146 - 165 °C
295 - 329 °F
Average value: 162 °C Grade Count:21
Overview of materials for Polypropylene, Fiber Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app..
Melting Point 156 - 165 °C
313 - 329 °F
10°C/min; ASTM D3418
Shanghai Ofluorine T-1 PVDF for coatings (DF-1)
Description: T-1 PVDF for coatings is solid powder, it can mixed with acrylic resin, additive, and become superior performance baking PVDF fluorocarbon coatings. Compared with other grade of PVDF, T..
Melting Point 161 - 165 °C
322 - 329 °F
ISO 3146
Borealis Borclean™ HC300BF Polypropylene Homopolymer for Capacitor Film
Borclean HC300BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC300BF does not contain slip, antiblock, antist..
Melting Point 161 - 165 °C
322 - 329 °F
ISO 3146
Borealis Borclean™ HC312BF Polypropylene Homopolymer for Capacitor Film
Borclean HC312BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC312BF does not contain slip, antiblock, antist..
Melting Point 161 - 165 °C
322 - 329 °F
ISO 3146
Borealis Borclean™ HC318BF Polypropylene Homopolymer for Capacitor Film
Borclean HC318BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC318BF does not contain slip, antiblock, antist..
Melting Point 162 - 165 °C
324 - 329 °F
ISO 3146
Borealis Daploy™ WF420HMS High Melt Strength Polypropylene for Extrusion Coating
Daploy WF420HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g..
Melting Point 162 - 165 °C
324 - 329 °F
DSC; ISO 3146
Borealis HB205TF Polypropylene
HB205TF is a low melt flow rate polypropylene homopolymer intended for extrusion, calendering and thermoforming. Its very good organoleptic properties allows this grade to be used with any master b..
Melting Point 161 - 165 °C
322 - 329 °F
DSC; ISO 3146
Borealis HC101BF Polypropylene Homopolymer
HC101BF is a polypropylene homopolymer. Applications: HC101BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, packa..
Melting Point 161 - 165 °C
322 - 329 °F
ISO 3146
Borealis HF420FB Polypropylene
HF420FB is a polypropylene homopolymer intended for fiber applications. HF420FB has been developed especially for applications like: staple fiber, continuous filaments, and spun bonded nonwovens.In..
Melting Point 161 - 165 °C
322 - 329 °F
DSC; ISO 3146
Borealis HG420FB Polypropylene
HG420FB is a polypropylene homopolymer intended for fiber applications. Applications: HG420FB has been developed especially for applications like spun bonded nonwovens.Information provided by Borea..
Melting Point 161 - 165 °C
322 - 329 °F
ISO 3146
Borealis HG455FB Polypropylene Homopolymer
HG455FB is a polypropylene homopolymer intended for fiber applications. Applications: fine filament count at high spinning speeds, spun bonded nonwovens, and POY production.Information provided by ..
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Total PPC 5720WZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 5720WZ is a nucleated impact copolymer with a Melt Flow index of 20 g/10 min.TOTAL Polypropylene 5720WZ is characterized by good stiffness, creep resistance, very ..
Melting Point 160 - 165 °C
320 - 329 °F
ATOFINA Method
Total PPC 5724 Polypropylene, Extra High Impact Copolymer
ATOFINA 5724 is characterized by a high fluidity offering a combination of processing and excellent impact properties in applications ranging from industrial to household.ApplicationATOFINA 5724 has..
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Total PPC 5946WZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 5946WZ is a nucleated impact copolymer with a Melt Flow index of 75 g/10 min.TOTAL Polypropylene 5946WZ is characterized by very low warpage, improved stiffness, a..
Melting Point 160 - 165 °C
320 - 329 °F
ATOFINA Method
Total PPC 4720 WZ Polypropylene, Impact Copolymer
ATOFINA 4720 is an impact copolymer. 4720 is characterized by a high fluidity offering a combination of east of processing and good mechanical properties.ApplicationATOFINA 4720 has been formulated..
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Total PPC 4720XWZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 4720XWZ is a nucleated impact copolymer with a Melt Flow index of 25 g/10 min.TOTAL Polypropylene 4720XWZ is characterized by improved stiffness, creep resistance,..
Melting Point 160 - 165 °C
320 - 329 °F
ATOFINA Method
Total PPC 4824WZ Polypropylene, Impact Copolymer
ATOFINA 4824WZ is a nucleated impact copolymer. 4824WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. It has been formulated for excellent ..
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Total PPC 4920WZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 4920WZ is a nucleated impact copolymer with a Melt Flow index of 105 g/10 min.TOTAL Polypropylene 4920WZ is characterized by excellent stiffness and impact resista..
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Total PPC 4944CWZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 4944CWZ is a nucleated and controlled rheology impact copolymer with a very high Melt Flow index of 50 g/10 min.TOTAL 4944CWZ is characterized by improved stiffnes..
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Total PPC 5945WZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 5945WZ is a nucleated impact copolymer with a Melt Flow index of 80 g/10 min.TOTAL Polypropylene 5945WZ is characterized by very low warpage, improved stiffness, a..
Melting Point 160 - 165 °C
320 - 329 °F
[10 K/min], ISO 11357
Eurotec® Tecolen® CP20 GB30 NL PPCP, 30% glass bead reinforced, natural
Information provided by Eurotec®
Melting Point 160 - 165 °C
320 - 329 °F
[10 K/min], ISO 11357
Eurotec® Tecolen® CP20 GR40 NL PPCP, 40% glass fiber reinforced, natural
Information provided by Eurotec®
Melting Point 160 - 165 °C
320 - 329 °F
[10 K/min], ISO 11357
Eurotec® Tecolen® CP30 NL MY PPCP, impact modified, heat & UV stabilized, natural
Information provided by Eurotec®
Melting Point 155 - 165 °C
311 - 329 °F
Arkema Group KYNAR® 461 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Melting Point 155 - 165 °C
311 - 329 °F
Arkema Group KYNAR® 301-F Polyvinylidene Fluoride Powder
Characteristics: Fine milled, white, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abra..
Melting Point 160 - 165 °C
320 - 329 °F
DSC
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade
TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.Benefits. 4170 forms tough films with high dart imp..
Melting Point 160 - 165 °C
320 - 329 °F
[10 K/min], ISO 11357
Eurotec® Tecolen® CP30 NL XA80 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
Melting Point 161 - 165 °C
322 - 329 °F
DSC; ISO 3146
Borealis HE465FB Polypropylene
HE465FB is a polypropylene homopolymer intended for fiber applications. Applications: high tenacity CF yarn. Additives: HE465FB gas fading free formulation.Information provided by Borealis AG
Melting Point 155 - 165 °C
311 - 329 °F
Arkema Group KYNAR® 201 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Copyright © lookpolymers.com All Rights Reserved