Thermal Properties Metric English Comments
Melting Point 172 °C
342 °F
Crystallinity by DSC; ASTM D 3418
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer  (discontinued **)
Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina..
Melting Point 172 °C
342 °F
DSC
Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding TPU properties.Uses: Cable jacket and tube/hos..
Melting Point 172 °C
342 °F
ASTM D3418
UBE UBESTA® 3030JI5L Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet SAE J844, DIN73378 HIPHLInformation provided by UBE.
Melting Point 172 °C
342 °F
Zeus PVDF Tubing
PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char..
Melting Point 172 °C
342 °F
By DSC
Toyobo PELPRENE™ P40H Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
Melting Point 172 °C
342 °F
By DSC
Toyobo PELPRENE™ P40H-05 Polyester TPE, Non-smell, Non-deposit
Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo.
Melting Point 172 °C
342 °F
By DSC
Toyobo PELPRENE™ P40U Polyester TPE, Weather-resistant
Features: Polyester TPE, Weather-resistantInformation provided by Toyobo.
Melting Point 172 °C
342 °F
DSC
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in..
Melting Point 172 °C
342 °F
ASTM D3418
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Melting Point <= 172 °C
<= 342 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ FL 00623 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00623 is a good coextrusion partner in extrusion coating, blown and cast film. Excellent sealing material with a very low seal initiation temperature. Availability: Africa & ..
Melting Point <= 172 °C
<= 342 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ UL 7511 Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra UL 7511 is a very high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt ad..
Melting Point 172 °C
342 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® XG5855 TPC-ET
Extrusion Grade
Melting Point 172 °C
342 °F
ASTM D3448
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products
Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent..
Melting Point 172 °C
342 °F
ASTM D3418
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA)
Information provided by Arkema Group
Melting Point 172 °C
342 °F
ISO 11357
Arkema Group Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Melting Point 172 °C
342 °F
ISO 11357
Arkema Group Pebax® 7033 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Melting Point 172 °C
342 °F
(Dry)
Arkema Group Pebax® 7033 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 70 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay..
Melting Point 172 °C
342 °F
10°C/min
Arkema Group Pebax® 7033 SN 01 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) hardness 70 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay..
Melting Point 172 °C
342 °F
ISO 11357
Arkema Group Pebax® 7033 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Melting Point 172 °C
342 °F
ASTM D789
Arkema Group PLATAMID® 8020 Copolyamide
Platamid® 8020 is a transparent, thermoplastic copolyamide designed for conversion by standard molding or extrusion techniques.Information provided by Arkema Group