Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 224 °C | 435 °F | ASTM D3418 |
Nylene® 9533 , 33% Glass Reinforced Nylon 6/12 Description: Nylene® 9533 is a 33% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resou.. |
|||
Melting Point | 224 °C | 435 °F | ASTM D3418 |
Nylene® 9543 , 43% Glass Reinforced Nylon 6/12 Description: Nylene® 9543 s a 43% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resour.. |
|||
Melting Point | 224 °C | 435 °F | ISO 3146 |
PolyOne Bergadur™ PB40 G20 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® S610SF BK851 PBT
(Unverified Data**) Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati.. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® SK612SF NC010 PBT
(Unverified Data**) Crastin® SK612SF is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PL471 45 Shore D, Injection Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP213G45 Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP2122G15VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP211 General Purpose PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP212G30VO G/F Reinforced & Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP213G15BL Glass Fiber Reinforced PBT Compound Resin b>Characteristics: G/F 15% reinforced, BLACKApplications: Impeller housingsInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin G/F 15% + Impact resistantApplications: SwitchesInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP213G20WBL Glass Fiber Reinforced & Weather Resistant PBT Compound Resin G/F 20% reinforced, weather resistanceApplications: Parts of electric lightInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP513 PBT Alloy Resin Excellent extrudable and SpinningApplications: Mono filamentInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP513UG PBT Alloy Resin Extrudable, delusteringApplications: Mono filamentInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP515FLBL High Impact PBT Alloy Resin High elastic, whether resistantApplications: WipersInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Pocan® DP 2004 000000 PBT PBT, non-reinforced, injection molding, halogen free flame retardant |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® BKV 30 FN00 000000 Nylon 6, 30% Glass Fiber PA6, injection molding grade, 30% glass fibers, UL94 V-0 at 0,75 mm , free of halogen and red phosphorus, glow wire flammability test max. 960°C |
|||
Melting Point | 224 °C | 435 °F | |
Techmer ES HiFill® PA6 GB15 L BK 15% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 15% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Good UV Resistance and LubricatedAppearance: BlackTPCI# .. |
|||
Melting Point | 224 °C | 435 °F | ASTM D3418 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Melting Point | 224 °C | 435 °F | ASTM D3418 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Melting Point | 224 °C | 435 °F | DSC Peak; JIS K7121 |
Goodfellow TPX® MX002O Polymethylpentene This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi.. |
|||
Melting Point | 224 °C | 435 °F | ASTM D3418 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Melting Point | 224 °C | 435 °F | ISO 11357-1/-3 |
Covestro Makroblend® KU 2-7912/5 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh flowhigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
Melting Point | 224 °C | 435 °F | ASTM DSC |
Cresset Powers Cress-Alon™ A3000 3.0 r.v. Film or Extrusion Grade Nylon 6, Dry As Molded Neat resin, for film or extrusion.Information provided by Cresset Powers Ltd. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® SK612SF BK591 PBT Crastin® SK612SF BK591 is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast .. |
|||
Melting Point | 224 °C | 435 °F | ISO 3146 |
Azoty Tarnow™ Alphalon™ E 40 T Nylon 6 A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™ |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610
(Unverified Data**) Zytel® RS 30G30HSL BK038A is a lubricated, heat stabilized, 30% glass fiber reinforced black polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on po.. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
(Unverified Data**) Zytel® RS 30G30L NC010 is a lubricated, 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer only). It was initia.. |