Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 55.0 - 90.0 °C | 131 - 194 °F | |
Kazanorgsintez NMPE-2 Low-Molecular Polyethylene Notes: Low-molecular polyethylene of high pressure polyethylene production. Application: Designed for use in the rubber industry, building industry, and other fields. Can also be used as compon.. |
|||
Melting Point | 88.0 - 90.0 °C | 190 - 194 °F | |
BASF Imidazole Formula: C3H4N2CAS: 288-32-4Description: Imidazole is a crystalline powder with an amine-like odor. It is soluble in water.Synonyms: 1,3-Diaza-2,4-cyclopentadiene, 1,3-Diazole, Imidazol, Methanimid.. |
|||
Melting Point | 87.0 - 90.0 °C | 189 - 194 °F | |
BASF 2,5-Dimethyl-2,5-hexanediol Formula: C8H18O2CAS: 110-03-2Description: Dimethylhexanediol is a colorless to yellow solid, and is odorless. It is soluble in water and easily soluble in alcohols and acetone.Synonyms: 2,5-Dimethy.. |