Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 99.0 °C | 210 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 3030 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 99.0 °C | 210 °F | Exxon Method |
ExxonMobil Escorene® LD-318 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Melting Point | 99.0 °C | 210 °F | Exxon Method |
ExxonMobil Escorene® LD-319 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Melting Point | 99.0 °C | 210 °F | Exxon Method |
ExxonMobil Escorene® LD-333 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.Applications: Prim.. |
|||
Melting Point | 99.0 °C | 210 °F | ASTM D3418 |
Petroquimica Triunfo Tritheva® TN 2007 EVA Copolymer The Tritheva TN 2007 resin is an Ethylene-Vinyl Acetate copolymer (EVA), developed to meet the multi-layer packaging needs where are required high strength, with high toughness, and excellent optica.. |
|||
Melting Point | 99.0 °C | 210 °F | DSC; ASTM D3418 |
DuPont Bynel® 30E671 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 99.0 °C | 210 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va.. |
|||
Melting Point | 99.0 °C | 210 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3120 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 7.5 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dr.. |
|||
Melting Point | 99.0 °C | 210 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film 9.5 wt% Acrylic Acid.Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.F.. |
|||
Melting Point | 99.0 °C | 210 °F | ASTM D3418 |
DuPont Trancend™ Extrusion Coating Sealant DuPont™ Trancend™ is an ethylene acrylic acid ionomer, expressly designed for extrusion coating, using a new generation of manufacturing technology. This new technology has allowed DuPont to produ.. |
|||
Melting Point | 99.0 °C | 210 °F | UBE method |
UBE UMERIT 1500F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Melting Point | 99.0 °C | 210 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 3930 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 99.0 °C | 210 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The.. |
|||
Melting Point | 99.0 °C | 210 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 11.5 wt% Methacrylic Acid.Nucrel® 1202HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment des.. |
|||
Melting Point | 99.0 °C | 210 °F | ASTM D3418, ISO 3146 |
DuPont™ Elvax® 3128-1 Ethylene Vinyl Acetate DuPont™ Elvax® 3128-1 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® .. |
|||
Melting Point | 99.0 °C | 210 °F | Dow Method (DSC) |
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP) AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi.. |
|||
Melting Point | 99.0 °C | 210 °F | Dow Method |
Dow AMPLIFY™ EA 100 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 100 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer.. |
|||
Melting Point | 99.0 °C | 210 °F | |
BASF Lucalen® A 3110 M Ethylene/Acrylate Copolymer Economical composite films together with PE-LD; primers for aluminum/steel composites; coatings for paper board, aluminum and steel (e.g. for pipes used to transport petroleum, gas, etc.)Data was co.. |
|||
Melting Point | 99.0 °C | 210 °F | |
BASF Lucalen® A 3110 M Q 244 Ethylene/Acrylate Copolymer Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 99.0 °C | 210 °F | |
BASF Lucalen® A 3110 M Q 270 Ethylene/Acrylate Copolymer Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 99.0 °C | 210 °F | |
BASF Lucalen® A 3120 M Ethylene/Acrylate Copolymer Suitable in similar manner as Lucalen A 2920 M or also as a material for coating aluminum, steel, paper and cardboard. Also for processing pipes for transporting petroleum, gas, etc.Data was collec.. |
|||
Melting Point | 99.0 - 108 °C | 210 - 226 °F | |
BASF Luwax® OA 2 Pastilles Description: Hard, emulsifiable polyethylene wax. Used to produce finely dispersed wax emulsions or polishes and many other products. Lubricant for processing PVC.Information provided by BASF |
|||
Melting Point | 99.0 °C | 210 °F | DSC; ASTM D3418 |
DuPont™ Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1802 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces.. |
|||
Melting Point | 99.0 °C | 210 °F | ASTM D3417- ISO 3146 |
DuPont Elvax® 880 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 880 is an ethylene-vinyl acetate copolymer resin containing slip and anti-block additives for use in industrial applications.Applications: Elvax® 880 resins can be used for the fo.. |