Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Not listed in the ASTM.Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 1018, Grade 33 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 1018, Grade 36 Type 1 and 2 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 570, Grade 30 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 570, Grade 36 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 607 Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 607 Class 2 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel Cold Rolled Carbon Steel, Bake Hardenable (BH 210), SAE J2340 Type 210 B Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel Cold Rolled Carbon Steel, Bake Hardenable (BH 250) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel Cold Rolled Carbon Steel, Commercial Steel (CS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel Cold Rolled Carbon Steel, Drawing Steel (DS Type B), Standard Grade DS is made by adding aluminum to the molten steel and may be used in drawing applications.Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F) steels are made by adding titanium and/or niobium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel Hot Rolled Carbon Steel, Drawing Steel with Boron (DS Type B), Standard Grade DS is made by adding aluminum and boron to the molten steel and may be used in severe drawing applications.Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel SAE J1392 040XLK or 040YLK, Grade 40 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel Type 1 & 2, Grade 33 Cold Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ZINCGRIP® 255, Grade 37 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ZINCGRIP® FORMABLE 50K / ASTM A1008 class 2 / SAE J1392 050 XLK, Grade 50 Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Steel, Bake Hardenable (BH 180) Brake Hardenable steels offer good formability and an increase in strength after paint bake.Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Interstitial Free (I-F®) steels are made by adding titanium and/or columbium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 21.0 - 93.0 °C |
0.115 BTU/lb-°F @Temperature 69.8 - 199 °F |
|
ATI Allegheny Ludlum K12® Dual Hardness Steel This is a roll bonded, dual hardness armor plate consisting of a high hardness front side to break up or flatten incoming projectiles while the back side functions to capture the projectile.The comp.. |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 1011, Grade 30 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 1011, Grade 36 Type 1 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 568 and A 635 Hot Rolled Carbon Steel, Structural Steel (SS) For conversion to A36 plateInformation provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ASTM A 570, Grade 45 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F) steels are made by adding titanium and/or columbium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel |
|||
Specific Heat Capacity | 0.481 J/g-°C @Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F @Temperature 122 - 212 °F |
|
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Dent Resistant (DR 210) Information provided by AK Steel |
|||
Specific Heat Capacity | 0.480 J/g-°C | 0.115 BTU/lb-°F | |
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small labora.. |
|||
Specific Heat Capacity | 0.482 J/g-°C @Temperature 200 °C |
0.115 BTU/lb-°F @Temperature 392 °F |
|
Special Metals INCOLOY® Alloy 903 A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a.. |