Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203 PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203RM PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 223R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 223S PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Specific Heat Capacity | 1.26 J/g-°C @Temperature 4.00 °C |
0.301 BTU/lb-°F @Temperature 39.2 °F |
ASTM E1269 |
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 243 PC 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 243 PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Specific Heat Capacity | 1.26 J/g-°C @Temperature 4.00 °C |
0.301 BTU/lb-°F @Temperature 39.2 °F |
ASTM E1269 |
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM E1269 |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 307E4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360A4861316 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 380A3V32818 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 380A4000015 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | |
ACC QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber QSil 216 is a two-part, clear, liquid silicone which will cure at room temperature or at elevated temperatures. It has a low viscosity, which allows for ease of flow around complex parts, providing .. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |