Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | (DSC, 10°C/min); DIN 51.007 |
Lubrizol Advanced Materials Pearlcoat® 125KW Thermoplastic Polyurethane Elastomer
(discontinued **) Pearlcoat® D125KW is a polyester-based aromatic TPU, supplied in form of white-colored pellets, combining hardness with excellent low-temperature flexibility.Applications: Pearlcoat® D125KW is us.. |
|||
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | DMTA |
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | DMTA |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | |
Mallard Creek Polymers ROVENE® 6140 SBR Latex ROVENE® 6140 is a carboxylated styrene-butadiene emulsion that has a very soft and resilient hand that can be used for upholstery backcoating to produce fabrics showing high seam strengths. Due t.. |
|||
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF) Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Glass Transition Temp, Tg | -28.0 - -28.0 °C | -18.4 - -18.4 °F | |
Zeon Chemicals Nipol® 1492P80 Nitrile Powder and Crumb Elastomer Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is .. |
|||
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | DSC |
Lubrizol Estane® 58252 Thermoplastic Polyurethane Type: Estane® 58252 is a 70A polyether-type thermoplastic polyurethane (TPU).Features: Formulated to have one of the highest MVT values within the thermoplastic polyurethane class. It is also amon.. |
|||
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | DSC |
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai.. |
|||
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | DSC |
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, AutomotiveDat.. |
|||
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | DSC |
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-45D ether-ether hybrid polyurethane elastomer has excellent low temperature properties, fast cycle time, and good resistance to fuel and oils. Applications include: C.. |
|||
Glass Transition Temp, Tg | -28.0 °C | -18.4 °F | Compound |
KKPC KOSYN SOL 5740 Solution Styrene Butadiene Rubber (S-SBR) Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It .. |