Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glass Transition Temp, Tg = -28.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
(DSC, 10°C/min); DIN 51.007
Lubrizol Advanced Materials Pearlcoat® 125KW Thermoplastic Polyurethane Elastomer  (discontinued **)
Pearlcoat® D125KW is a polyester-based aromatic TPU, supplied in form of white-colored pellets, combining hardness with excellent low-temperature flexibility.Applications: Pearlcoat® D125KW is us..
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
DMTA
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer  (Unverified Data**)
Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General ..
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
DMTA
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer  (discontinued **)
Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i..
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
Mallard Creek Polymers ROVENE® 6140 SBR Latex
ROVENE® 6140 is a carboxylated styrene-butadiene emulsion that has a very soft and resilient hand that can be used for upholstery backcoating to produce fabrics showing high seam strengths. Due t..
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
ASTM E1356
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
ASTM E1356
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF)
Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Glass Transition Temp, Tg -28.0 - -28.0 °C
-18.4 - -18.4 °F
Zeon Chemicals Nipol® 1492P80 Nitrile Powder and Crumb Elastomer
Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is ..
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
ASTM D4065
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers.
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
DSC
Lubrizol Estane® 58252 Thermoplastic Polyurethane
Type: Estane® 58252 is a 70A polyether-type thermoplastic polyurethane (TPU).Features: Formulated to have one of the highest MVT values within the thermoplastic polyurethane class. It is also amon..
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
DSC
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane
Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai..
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
DSC
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)  (discontinued **)
Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, AutomotiveDat..
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
DSC
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)  (discontinued **)
Description: PELLETHANE® 2104-45D ether-ether hybrid polyurethane elastomer has excellent low temperature properties, fast cycle time, and good resistance to fuel and oils. Applications include: C..
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
Compound
KKPC KOSYN SOL 5740 Solution Styrene Butadiene Rubber (S-SBR)
Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It ..
Copyright © lookpolymers.com All Rights Reserved