Polymer Property : Glass Transition Temp, Tg = -58.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
ISO 11357-1
Murtfeldt Murytal® C Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
ISO 11357-1
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
ISO 11357-1
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive
Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•..
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
ISO 11357-1
Murtfeldt Murytal® H Acetal Homopolymer
In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it..
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
10°C/min; ISO 11357-1/-2
DuPont Performance Polymers Hytrel® 4069 TPC-ET  (Unverified Data**)
Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection..
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
DSC, 10ºC/min; DIN 51.007
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 163K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE..
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
Styron XU 36535.00 Formulated SB
Performance Features: ENVERSAâ„¢ Cushion Technology, excellent recovery, cushion, excellent acoustic propertiesApplications: Sound DampeningNorth AmericaInformation provided by Styron
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
ASTM D3418
DuPont Elvaloy® HP4051 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
Wanhua Chemical Wanthane® WHT-8280 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
DSC
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane
Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio..
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
DSC
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compoundUses: Extrusion – Wire and cable and general application where flame retardant properties are neededAvailable in Americas, Europe, Middle East, Africa,..
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
DSC
Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane
Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion along with wide processing window for extrusion and low surface tack.Uses: Blown and flat die/cast..
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
DSC
Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane
Features: Good Elasticity – High melt flow for easy processingUses: Extrusion – Wire and cable, general extrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provi..
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
10°C/min; ISO 11357-1/-2
DuPont Performance Polymers Hytrel® 4053FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
10°C/min; ISO 11357-1/-2
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
10°C/min; ISO 11357-1/-2
DuPont Performance Polymers Hytrel® 4056P Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer in Powder FormInformation provided by DuPont Performance Polymers
Glass Transition Temp, Tg <= -50.0 °C
<= -58.0 °F
ASTM D3418
Arkema Group Pebax® MV1074 Polyether Block Amide
Glass Transition Temp, Tg <= -50.0 °C
<= -58.0 °F
ASTM D3418
Arkema Group Pebax® MV1657 Polyether Block Amide
Glass Transition Temp, Tg <= -50.0 °C
<= -58.0 °F
Cured property; Perkin Elmer TM-2
Aptek 2313-PMF Hybrid Epoxy Adhesive
Snap-cure, silver-filled; long pot-life/stable viscosity-excellent for robotics. Thermal shock resistant.Production-oriented, snap-cure technology for surface mount applications-allows cure during s..
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
10°C/min
Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema.
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
DSC
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane
Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection..