Thermal Properties Metric English Comments
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
ISO 11359-2:1999
Nylacast POM C Acetal Copolymer
The copolymer grade is the ideal combination of strength, stiffness and wears resistance. It absorbs very little moisture, is easily machinable and is genuinely porosity-free making it the preferred..
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
ISO 11359-2:1999
Global EPP POM C Acetal Copolymer
Polyacetals are highly crystalline thermoplastics, characterised by their high mechanical strength, rigidity and impact resistance. Acetal absorbs very little moisture, enabling the product to maint..
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
Wanhua Chemical Wanthane® WHT-8170 Polyether-Based TPU
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
DSC
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified
Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol..
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
DSC
Lubrizol Estane® AG 4350 Thermoplastic Polyurethane
Type: Estane® AG 4350 is a polyether based aliphatic polyurethane specifically formulated to be used as an adhesive interlayer without the need for a glass surface primer. This polymer is designed..
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
DSC
Lubrizol Estane® AG 4950 Thermoplastic Polyurethane
Type: Estane® AG 4950 is a polyether based aliphatic thermoplastic polyurethane (TPU) specifically formulated to be used as an adhesive interlayer in transparencies for electronic displays, aerospa..
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
DSC
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane
Type: Estane® AG 8451 is a polyether based aliphatic (TPU) specifically formulated to be used as an adhesive interlayer film. AG-8451 is an excellent general purpose polymer for all optical allpha..
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
10°C/min; ISO 11357-1/-2
DSM Arnitel® EL630 63 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
ASTM D3418
Ensinger Tecaform™ MT Acetal, Medical Grade (POM)
TECAFORM® MT is Ensinger's specially formulated medical grade acetal. The material is resistant to multiple cleaning and disinfection agents, and to a number of solvents. It can be steam sterilized..
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
Cured property; JMTP P-200
Aptek 2120 PMF Low modulus urethane staking compound
Premixed-frozen, low modulus urethane staking compoundAPTEK 2120-PMF is a one component, premixed-frozen, thixotropic, electrically insulating soft urethane adhesive. It was designed for the stakin..
Glass Transition Temp, Tg <= -60.0 °C
<= -76.0 °F
Cured property; Perkin Elmer TS-2
Aptek 2214-A/B Low modulus urethane ESD coating/adhesive
Space Grade, Low modulus urethane ESD coating/adhesiveAPTEK is a carbon-filled, thixotropic, two component, electrically conductive, flexible urethane coating/adhesive designed to dissipate an elect..
Glass Transition Temp, Tg <= -60.0 °C
<= -76.0 °F
Cured property; JMTP P-200
Aptek 2312-PMF Electrically conductive, low modulus adhesive
Premixed-frozen, electrically conductive, low modulus adhesiveAPTEK 2312-PMF is a one component, premixed-frozen, silver filled, electrically conductive soft paste adhesive. It is designed to bond m..
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
Cured property; JMTP P200
Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating
Room temperature curing, low modulus urethane conformal coatingAPTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the e..
Glass Transition Temp, Tg -60.0 °C
-76.0 °F
Glass Transition Temperature (10°C/min); ISO 11357-1/-2
DSM Arnitel® EL630 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Copyright © lookpolymers.com All Rights Reserved