Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | ISO 11359-2:1999 |
Nylacast POM C Acetal Copolymer The copolymer grade is the ideal combination of strength, stiffness and wears resistance. It absorbs very little moisture, is easily machinable and is genuinely porosity-free making it the preferred.. |
|||
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | ISO 11359-2:1999 |
Global EPP POM C Acetal Copolymer Polyacetals are highly crystalline thermoplastics, characterised by their high mechanical strength, rigidity and impact resistance. Acetal absorbs very little moisture, enabling the product to maint.. |
|||
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | |
Wanhua Chemical Wanthane® WHT-8170 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | DSC |
Lubrizol Estane® AG 4350 Thermoplastic Polyurethane Type: Estane® AG 4350 is a polyether based aliphatic polyurethane specifically formulated to be used as an adhesive interlayer without the need for a glass surface primer. This polymer is designed.. |
|||
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | DSC |
Lubrizol Estane® AG 4950 Thermoplastic Polyurethane Type: Estane® AG 4950 is a polyether based aliphatic thermoplastic polyurethane (TPU) specifically formulated to be used as an adhesive interlayer in transparencies for electronic displays, aerospa.. |
|||
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | DSC |
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane Type: Estane® AG 8451 is a polyether based aliphatic (TPU) specifically formulated to be used as an adhesive interlayer film. AG-8451 is an excellent general purpose polymer for all optical allpha.. |
|||
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | 10°C/min; ISO 11357-1/-2 |
DSM Arnitel® EL630 63 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | ASTM D3418 |
Ensinger Tecaform™ MT Acetal, Medical Grade (POM) TECAFORM® MT is Ensinger's specially formulated medical grade acetal. The material is resistant to multiple cleaning and disinfection agents, and to a number of solvents. It can be steam sterilized.. |
|||
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | Cured property; JMTP P-200 |
Aptek 2120 PMF Low modulus urethane staking compound Premixed-frozen, low modulus urethane staking compoundAPTEK 2120-PMF is a one component, premixed-frozen, thixotropic, electrically insulating soft urethane adhesive. It was designed for the stakin.. |
|||
Glass Transition Temp, Tg | <= -60.0 °C | <= -76.0 °F | Cured property; Perkin Elmer TS-2 |
Aptek 2214-A/B Low modulus urethane ESD coating/adhesive Space Grade, Low modulus urethane ESD coating/adhesiveAPTEK is a carbon-filled, thixotropic, two component, electrically conductive, flexible urethane coating/adhesive designed to dissipate an elect.. |
|||
Glass Transition Temp, Tg | <= -60.0 °C | <= -76.0 °F | Cured property; JMTP P-200 |
Aptek 2312-PMF Electrically conductive, low modulus adhesive Premixed-frozen, electrically conductive, low modulus adhesiveAPTEK 2312-PMF is a one component, premixed-frozen, silver filled, electrically conductive soft paste adhesive. It is designed to bond m.. |
|||
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | Cured property; JMTP P200 |
Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating Room temperature curing, low modulus urethane conformal coatingAPTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the e.. |
|||
Glass Transition Temp, Tg | -60.0 °C | -76.0 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Arnitel® EL630 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |