Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 121 °C | 250 °F | 10°C/min test |
Polimeri Europa SINKRAL C350 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-08-16-25 Heat resistant injection moulding grade. Combines good flow with toughness and high thermal charac.. |
|||
Glass Transition Temp, Tg | 121 °C | 250 °F | DSC |
Kolon NOPLA® KE931 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Glass Transition Temp, Tg | 121 °C | 250 °F | Dry |
Hexcel® HexPly® F155 Epoxy Resin HexPly® F155 is an advanced modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness and adhesive properties. HexPly.. |
|||
Glass Transition Temp, Tg | 121 °C | 250 °F | Dry |
Hexcel® HexPly® F522 Epoxy Resin HexPly® F522 is an advanced, modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness, excellent hot-wet properties .. |
|||
Glass Transition Temp, Tg | 121 °C | 250 °F | DSC |
DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge Teonex® Q51 is biaxially oriented polyethylene naphthalate (PEN) film. It is slightly hazy with excellent handling properties for general purpose. It is commercially available in nominal 48 - 1000 .. |
|||
Glass Transition Temp, Tg | 121 °C | 250 °F | DSC |
DuPont Teijin Films Teonex® Q83 Polyester Film, 200 Gauge Teonex® Q83 is biaxially oriented, slightly hazy polyethylene naphthalate (PEN) film with excellent handling properties and high dimensional stability. It is commercially available in 100, 200 and .. |
|||
Glass Transition Temp, Tg | 121 °C | 250 °F | dry |
Henkel Hysol EA 9628 Film Adhesive First generation, modified epoxy film, good stress, environmental resistance and structural propertiesApplications: Composite Bonding, Metal & Honeycomb BondingData from .060 psf, 300 g/m2 |