Polymer Property : Glass Transition Temp, Tg = 155 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -5.00 - 155 °C
23.0 - 311 °F
Average value: 74.0 °C Grade Count:80
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..
Glass Transition Temp, Tg 145 - 155 °C
293 - 311 °F
DMA
Hexcel® HexPly® 1458 160°C-180°C Curing Epoxy Matrix
HexPly® 1458 is a self-extinguishing and self-adhesive modified epoxy resin system for monolithic and sandwich structures. HexPly® 1458 has excellent temperature and moisture resistance. It has a ..