Polymer Property : Glass Transition Temp, Tg = 245 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 245 °C
473 °F
Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin  (discontinued **)
Supradel HTS-2401 is a high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature o..
Glass Transition Temp, Tg 245 °C
473 °F
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2..
Glass Transition Temp, Tg 245 °C
473 °F
Solvay Specialty Polymers Supradel® HTS-2430 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of ..
Glass Transition Temp, Tg 245 °C
473 °F
Solvay Specialty Polymers Supradel® HTS-2400 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2400 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and heat deflection temperature of 235°C, this resin extends the..