Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 1000F PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be sup.. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 1010F PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 2100R PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 2110R PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 2210K PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 2212R PEI (Europe-Africa-Middle East) 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 2300F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact compliant. Effective June, 2007 this grade will no longer be supported with .. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 2300R PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 2300R PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 2310F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 2312 PEI (Europe-Africa-Middle East) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 2410R PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 4000 PEI (Asia Pacific) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 4211 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM HU1110 PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM HU2210 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM HU2310 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics Ultem PW2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 1000P PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) in 350 micron powder. Resin is RoHS compliant. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics Ultem 1010KM PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM 1000EF PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS. US FDA and EU Food Contact compliant. |
|||
Glass Transition Temp, Tg | 217 °C | 423 °F | |
SABIC Innovative Plastics ULTEM AUT200 PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperatu.. |