Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Ovation Polymers Uttap SF 600 Polyethersulfone Polyether Sulfone Resin-Medium Viscosity, unreinforced standard grade for Easy Injection Molding.Information provided by Ovation Polymers |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Ovation Polymers UTTAP™ SF 50030 GF Polyether Sulfone, 30% Glass Fiber Excellent chemical and electrical resistance, high stiffness, modulus and HDTAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Gharda Chemicals Gafone™ 3610GM20 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5001 PEI Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Asia Pacific) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Asia Pacific) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Europe-Africa-Middle East) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5111 PEI 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS com.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5301 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5711 PEI 15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3418 |
Westlake Plastics PES film Made from ULTRASON® E Polyethersulfone Resin High heat deflection and continuous use temperature. Exceptional tensile and flexural strength. High dielectric strength. Exceptional mechanical properties. Dimensionally stable at varying tempera.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-2 |
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-2 |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-3 |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-2 |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-2 |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Gharda Chemicals Gafone™ B2315GF Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | Average value: 225 °C Grade Count:3 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | Average value: 225 °C Grade Count:3 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | DSC |
Gharda Chemicals GAFONE™ 3430GF PES, Glass Fiber-Reinforced