Thermal Properties Metric English Comments
Glass Transition Temp, Tg 230 °C
446 °F
Laminate; post cure
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Glass Transition Temp, Tg 230 °C
446 °F
Laminate; post cure
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Glass Transition Temp, Tg 230 °C
446 °F
Laminate; post cure
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 3k 5HS Carbon Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Glass Transition Temp, Tg 230 °C
446 °F
Laminate; post cure
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Glass Transition Temp, Tg 230 °C
446 °F
Laminate; post cure
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Glass Transition Temp, Tg 230 °C
446 °F
DMA (SSYS)
RedEye On Demand Polyphenylsulfone (PPSF), Rapid Prototyping Material
Polyphenylsulfone (PPSF) is a durable high-end thermoplastic that can be used in the toughest applications. Parts built in PPSF can handle heat near 400°F (204°C), it resists petroleum products, a..
Glass Transition Temp, Tg 230 °C
446 °F
DMA (SSYS)
Stratasys® Polyphenylsulfone
PPSF/PPSU (polyphenylsulfone) material has the greatest strength, heat and chemical resistance of all Stratasys materials - ideal for aerospace, automotive and medical applications. Stratasys FDM (F..
Glass Transition Temp, Tg 230 °C
446 °F
DAM (SSYS)
Proto3000 PPSF Fused Deposition Modeling Polymer
Description: PPSF/PPSU (polyphenylsulfone) material has the greatest heat and chemical resistance of all Fortus materials - ideal for aerospace, automotive and medical applications. PPSF parts manuf..