Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glass Transition Temp, Tg = 7.00 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 7.00 °C
44.6 °F
Film; DSC
Solvay Specialty Polymers Diofan® A602 Polyvinylidene Chloride (PVDC)  (discontinued **)
DIOFAN® A602 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. It features strong barrier prop..
Glass Transition Temp, Tg 7.00 °C
44.6 °F
Mallard Creek Polymers ROVENE® 6087 Styrene-Acrylic Emulsion
ROVENE® 6087 is a high solids, low VOC styrene-acrylic copolymer emulsion that provides outstanding wet strength and moisture barrier properties.APPLICATIONS: ROVENE® 6087 typical applications..
Glass Transition Temp, Tg 7.00 °C
44.6 °F
Mallard Creek Polymers ROVENE® 6487 Styrene-Acrylic Emulsion
ROVENE® 6487 is a high solids, low VOC styrene-acrylic copolymer emulsion that provides outstanding wet strength and moisture barrier properties.APPLICATIONS: ROVENE® 6487 typical applications..
Glass Transition Temp, Tg 7.00 °C
44.6 °F
DSC heating rate = -10° C/min
Kuraray SEPTON® H5127
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
Glass Transition Temp, Tg 7.00 °C
44.6 °F
DSC
Solvay Specialty Polymers Diofan® A 602 Polyvinylidene Chloride (PVDC)
Diofan® A 602 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances.It features strong barrier pr..
Glass Transition Temp, Tg 7.00 °C
44.6 °F
Styron DL 238NA Carboxylated SB
Performance Features: Strong bonding with clays and fillersApplications: General Purpose AdhesiveNorth AmericaInformation provided by Styron
Glass Transition Temp, Tg 7.00 °C
44.6 °F
Styron Modifier A/NA SB Latex
Performance Features: Excellent alkaline stability, excellent adhesion and strength, freeze/thaw stability, controlled air entrainment, meets FHWA RD-78-35Applications: Modified ConcreteNorth Americ..
Glass Transition Temp, Tg 7.00 °C
44.6 °F
Styron DL 2703LA Carboxylated SB
Performance Features: Excellent bonding, high film elongation, heat sealable, low odor, high water resistanceApplications: General Purpose AdhesiveLatin America/South AmericaInformation provided by ..
Glass Transition Temp, Tg 7.00 °C
44.6 °F
Onset
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro..
Glass Transition Temp, Tg 7.00 - 16.0 °C
44.6 - 60.8 °F
Average value: 12.8 °C Grade Count:8
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..
Glass Transition Temp, Tg 7.00 °C
44.6 °F
Styron Latex DL 2703LA Carboxylated SB
Performance Features: Excellent binding strength and durabilityApplications: Dust Control and Soil StabilizationLatin America/South AmericaInformation provided by Styron
Glass Transition Temp, Tg 7.00 °C
44.6 °F
Styron Modifier A SB Latex
Performance Features: Excellent alkaline stability, excellent adhesion and strength, freeze/thaw stability, controlled air entrainment, meets FHWA RD-78-35Applications: Latex Modified Concrete (LMC)..
Glass Transition Temp, Tg 7.00 °C
44.6 °F
Mallard Creek Polymers ROVENE® 4457 SBR Latex
ROVENE® 4457 is a highly carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is crosslinkable with extern..