Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glass Transition Temp, Tg = 775 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 413 °C
775 °F
ASTM D3418
Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet)
Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI ..
Copyright © lookpolymers.com All Rights Reserved