Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 95.0 °C | 203 °F | |
NextGen Adhesives P907-04 Fiber Optic Adhesive Description: NGAC P907-04 is a low viscosity and room temperature curing adhesive specifically formulated for fiber optic terminations.Advantages and Applications: Uses include the termination of si.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | DSC |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | 10°C/min test |
Polimeri Europa EDISTIR N1670 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,095-06 General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIP.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | 10°C/min test |
Polimeri Europa EDISTIR N1671 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,095-06 General purpose polystyrene with good flow and good heat resistance for rapid set-up. To be used in injection mol.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | ASTM D7426 |
Perstorp Compounds Akestra™ 90 Thermoplastic Copolyester Akestra™ is a thermoplastic with a sparkling glass-like appearance. It can be used as a polystyrene alternative for heat resistant thin wall containers, a polycarbonate alternative for durable “di.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | |
Eastman Tenite 105-28 Cellulose Acetate
(discontinued **) 28% Plasticized ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | wet, 175°C cure |
Henkel Hysol EA 9695 Film Adhesive Second generation, low flow, composite bonding film; excellent environmental resistance. Composite structure repair, cure and co-cure with composite laminates. Qualified to Airbus. Data from .050 ps.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | wet |
Henkel Hysol EA 9895 WPP Peel Ply Pre-impregnated, polyester peel ply product supplied in film form. Specially designed resin system capable of curing at 350°F / 177°C. Compatible with state-of-the-art composite prepreg resin .. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | |
Lucite International Elvacite ® 4045 Acrylic Resin Elvacite® 4045 is a medium molecular weight methyl methacrylate polymer. It is designed for use in solvent based screen printing inks, but can be used in a variety of ink formulations.Information.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | DSC |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | Ultimate Tg |
Tra-Con Tra-Bond 2119 Low Viscosity Glass Laminating Adhesive TRA-BOND 2119 is a crystal clear adhesive specifically designed for bonding glass to glass and glass to plastics. It also yields a high lap shear strength to metals and ceramics. This system cures t.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | Ultimate Tg |
Tra-Con Tra-Bond 2126 Black Opaque Epoxy Adhesive TRA-BOND 2126 is recommended for those modern photographic, industrial, and laboratory bonding and laminating applications where an easy-to-use, black (opaque) epoxy adhesive system with high perfor.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | DMA |
Hexcel® HexPly® ES/EH 84 120°C Curing Epoxy Matrix HexPly® ES/EH 84 matrix is a structural epoxy resin for tubular parts designed for low pressure curing in the manufacture of sports goods and for industrial applications. It is ideal for the follow.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | Ultimate Tg |
Tra-Con Tra-Bond F113SC BLK High Tg Fiber Optic Epoxy Adhesive TRA-BOND F113SC BLK is a fiber optic adhesive used for terminating ALL types of fiber optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | Ultimate Tg |
Tra-Con Tra-Bond F113SC High Tg Fiber Optic Epoxy Adhesive TRA-BOND F113SC is a room temperature curing, high Tg and low viscosity adhesive formulated for terminating ALL TYPES of fiber optic connectors. It has also been used for bonding LED displays, lense.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | Ultimate Tg |
Tra-Con Tra-Bond GA47-2LV Instrument Adhesive TRA-BOND GA47-2LV low viscosity adhesive is designed for guidance instrument applications. This adhesive exhibits excellent compatibility with conventional gyro flotation fluids. TRA-BOND GA47-2LV a.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | Ultimate Tg |
Tra-Con Tra-Bond F131 High Tg Room Temperature Cure Fiber Optic Adhesive TRA-BOND F131 is a fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C thus .. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | Wet |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix HexPly® M49 is a 120°C curing toughened epoxy matrix with good impact resistance suitable for use in performance cars. The matrix is highly tolerant of a wide variety of production techniques and .. |
|||
Glass Transition Temp, Tg | >= 95.0 °C | >= 203 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind.. |
|||
Glass Transition Temp, Tg | >= 95.0 °C | >= 203 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy Product Description: EPO-TEK® 354 is a two component, high Tg epoxy designed for semiconductor packaging in medical, fiber optic and optoelectronic assemblies. It is an electrically and thermally i.. |
|||
Glass Transition Temp, Tg | >= 95.0 °C | >= 203 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.Advantages & Application Notes:.. |
|||
Glass Transition Temp, Tg | >= 95.0 °C | >= 203 °F | Post-Cure Dynamic Scan 20200°C; Ramp -40200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® OG142 UV Cure Optical Epoxy Material Description: A single component, UV curable epoxy, designed for adhesive, sealing, and encapsulating applications found in semiconductor, electro-optics, fiber optics, medical, and scientif.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | |
Epoxyset Epoxiohm EO-38M-3 Electrically Conductive Epoxy Adhesive EO-38M-3 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management appl.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | |
Atom Adhesives AA-BOND F131 Epoxy Adhesive AA-BOND F131 is two parts fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. AA-BOND F131 produces a typical .. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | cured |
Atom Adhesives AA-BOND F156 Epoxy Adhesive AA-BOND F156 is a black, solvent free thixotropic epoxy recommended for high quality photographic industry, laminating, production and repair applications where a room temperature cure optically opa.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | |
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri.. |
|||
Glass Transition Temp, Tg | 95.0 - 108 °C | 203 - 226 °F | Average value: 102 °C Grade Count:7 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | |
Lucite International Elvacite ® 2021 Acrylic Resin Elvacite® 2021 is a high molecular weight methyl methacrylate polymer. It is used in barrier coatings for vinyl. Its high molecular weight provides excellent abrasion resistance.Information provide.. |
|||
Glass Transition Temp, Tg | 95.0 °C | 203 °F | |
Lucite International Elvacite ® 2021E Acrylic Resin Elvacite® 2021E is a high molecular weight methyl methacrylate. It provides a balance of solubility and hardness. It is used in migration barrier top coating for vinyl substrates. It is also used t.. |