Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C

@Thickness 6.40 mm
194 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics GELOY CR7020 ASA
ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact.
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C

@Thickness 6.40 mm
194 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific)
ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact.
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C

@Treatment Temp. 60.0 °C,
Thickness 3.18 mm
194 °F

@Treatment Temp. 140 °F,
Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ HTX E1502 Polyvinyl Chloride Alloy (PVC Alloy)
VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C

@Thickness 3.18 mm
194 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ HTX Ultra LA426 Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426 Black 2880.Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C

@Thickness 3.18 mm
194 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert..
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C

@Thickness 3.17 mm
194 °F

@Thickness 0.125 in
Unannealed; ASTM-D648
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C

@Thickness 3.20 mm
194 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL HIPS3190 HIPS
Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only.
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C

@Thickness 6.40 mm
194 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific)
ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL.