Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 91.1 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.1 °C

@Thickness 3.18 mm
196 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ HTX Ultra LA425 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors below 50L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Ductile/Brittle transition as measured by Instrumented Impact is 5 de..
Deflection Temperature at 0.46 MPa (66 psi) 91.1 °C

@Thickness 3.18 mm
196 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ HTX Ultra LA426 Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426 Black 2880.Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 91.1 °C

@Thickness 3.18 mm
196 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert..
Deflection Temperature at 0.46 MPa (66 psi) 91.1 °C

@Thickness 3.18 mm
196 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert..
Deflection Temperature at 0.46 MPa (66 psi) 91.1 °C

@Thickness 3.18 mm
196 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert..