Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 162 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 3.18 mm
162 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid)
Physical properties based on Geon L6607 white 1363Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M3890 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5000 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5015 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5100 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5200 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5700 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not..
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Fittings 210(HR) Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Fittings 210(HS) Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Fittings 87322 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Unannealed; ASTM-D648
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..