Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 1.17 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 2.10 - 225 µm/m-°C
1.17 - 125 µin/in-°F
Average value: 82.5 µm/m-°C Grade Count:3
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
CTE, linear, Transverse to Flow 2.10 µm/m-°C

@Temperature 20.0 °C
1.17 µin/in-°F

@Temperature 68.0 °F
Goodfellow Carbon/Epoxy Composite Sheet
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.
Copyright © lookpolymers.com All Rights Reserved