Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS (Asia Pacific) CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS (Asia Pacific) PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM6220 PC (Asia Pacific) CYCOLOY CM6220 resin is a mineral filled grade featuring of high modulus (6GPa), good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall fla.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -20.0 - 150 °C |
40.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Asia Pacific) PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -20.0 - 150 °C |
40.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC Available in a wide range of colors. Recommended for unpainted exterior/high heat/high impact applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® BM5225X PC (Asia Pacific) BM5225X resin is a mineral filled grade featuring of high modulus, good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance .. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Asia Pacific) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DI001E PC (Europe-Africa-Middle East) LNP* Lubricomp* DI001E is a compound based on Polycarbonate resin containing Silicone. Added features include: Internally Lubricated, Easy Molding. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFL42 PC LNP* Lubricomp* DFL-4042 a compound based on Polycarbonate resin containing 10% Glass Fiber, 20% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP QFN16 PA 6/10 LNP* LUBRICOMP* QFN16 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 5% MOS2. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp UL004AS PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, countaining PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DX12411C PC LNP* STAT-KON* DX12411C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM Test |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp PB00A PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PB00A is a compound based on PA 6 resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP QC006I PA 6/10 LNP THERMOCOMPâ„¢ QC006I is a compound based on Nylon 6/10 containing 30% Carbon Fiber. Added features of this grade include: High Impact. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl GTX GTX8110 PPE+PA (Europe-Africa-Middle East) GTX8110 is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaksThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V8090 PBT+PET (Europe-Africa-Middle East) 50% Glass Fiber Reinforced PBT-PET resin |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3006 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® T80 XG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Opt.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® UT-1018 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingSheet extrusionInformation provided by Bayer Polymers.As of 1 .. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR NC010 is a 35% glass reinforced toughened heat stabilized lubricated high performance polyamide resin. It is also a P.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide PB00A PA6, 50% Glass Bead Filled, Injection Molded Staramide PB00A is a 50% Glass Bead Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |