Polymer Property : CTE, linear, Transverse to Flow = 47.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics EXTEM UH1006 TPI Blend
High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha..
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical Resistant
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics EXTEM UH1006M TPI Blend
High heat amorphous TPI Blend, Chemical Resistant
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical Resistant
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics EXTEM UH1016 TPI Blend
High heat amorphous TPI Blend, Chemical Resistant, High Flow
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant, High Flow
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical Resistant, High Flow
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics Extem UH1016M TPI Blend
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics Extem UH1016M TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 831
SABIC Innovative Plastics EXTEM UH1026 TPI Blend
High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 20.0 °C
26.1 µin/in-°F

@Temperature 68.0 °F
TMA; ASTM E831
LNP Lubricomp® EL-4030 Polyetherimide, PTFE Additive  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 °C
26.1 µin/in-°F

@Temperature 73.4 °F
ASTM D696
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Crystalline  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 °C
26.1 µin/in-°F

@Temperature 73.4 °F
ASTM D696
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 °C
26.1 µin/in-°F

@Temperature 73.4 °F
ASTM D696
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Crystalline  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear, Transverse to Flow 47.0 µm/m-°C
26.1 µin/in-°F
Idemitsu Kosan Xarec® EA 513 SPS, 30% Glass Filled
CTE, linear, Transverse to Flow 47.0 µm/m-°C
26.1 µin/in-°F
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI
LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DX11411 PC
LNP* STAT-KON* DX11411 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
26.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON UEF26AS PPA (Europe-Africa-Middle East)
LNP* Stat-kon* UEF26AS is a compound based on Polyphthalamide resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP JF003E PES
LNP* THERMOCOMP* JF003E is a compound based on Polyethersulfone resin containing 15% Glass Fiber. Added features of this material include: Easy Molding.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
26.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Europe-Africa-Middle East)
LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 20.0 °C
26.1 µin/in-°F

@Temperature 68.0 °F
Covestro Makroblend® UT-620 G Polycarbonate + Polyester Blend
Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe..
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
26.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOTUF OF008EI PPS (Europe-Africa-Middle East)
LNP* Thermotuf* OF008EI is a compound based on PPS-Linear resin, containing Glass Fiber. Added features include : High Impact and Easy Molding.