Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 52.0 - 95.0 µm/m-°C
28.9 - 52.8 µin/in-°F
Average value: 72.3 µm/m-°C Grade Count:5
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
CTE, linear, Transverse to Flow 52.0 - 69.0 µm/m-°C
28.9 - 38.3 µin/in-°F
Average value: 58.0 µm/m-°C Grade Count:3
Overview of materials for Phenolic, Novolac, Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu..
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP OCL13XXP PPS - LINEAR (Europe-Africa-Middle East)
LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP UX05051 PPA (Europe-Africa-Middle East)
Internally lubricated Polyphthalamide compound, containing Glass Fiber and PTFE. Added features include Heat Stabilized, Flame Retardant and Hot Water Moldable
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX05301C PC
LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic..
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon OCL13 PPS - LINEAR (Europe-Africa-Middle East)
LNP* Stat-kon* OCL13 is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for..
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON OCL13XXP PPS - LINEAR (Europe-Africa-Middle East)
LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
28.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP AF004XXY ABS
LNP* Thermocomp* AF004XXY is a compound based on ABS containing 20% glass fiber.
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
28.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP AX02749 ABS
LNP* THERMOCOMP* AX02749 is a compound based on ABS containing proprietary fillers.
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP OF006A PPS (Europe-Africa-Middle East)
LNP* Thermocomp* OF-1006 is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP UF009AS PPA (Europe-Africa-Middle East)
LNP* Thermocomp* UF009AS is a compound based on Polyphthalamide resin containing Glass Fiber.
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP UF009AXP PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF009AXP is a compound based on Polyphthalamide resin containing 45% Glass Fiber.
CTE, linear, Transverse to Flow 52.0 µm/m-°C
28.9 µin/in-°F
ASTM E831
Sumitomo Bakelite North America RX® 525 Cellulose Reinforced Phenolic Novolac
RXÂ 525 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for parts requiring moderate toughness. It is designed to meet the requirements of ASTM D-594..
CTE, linear, Transverse to Flow 52.0 µm/m-°C
28.9 µin/in-°F
TMA
Vyncolit A2710 Glass Fiber Reinforced Novolac Phenolic
Vyncolit A2710 is a glass fiber reinforced phenolic molding compound with excellent mechanical and thermal properties.Information provided by Sumitomo Bak North America, Inc.
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature 20.0 °C
28.9 µin/in-°F

@Temperature 68.0 °F
Covestro Bayblend® KL 1-1427 Polycarbonate/ABS Blend
Glass fiber reinforced grade (30%) with high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – ..
CTE, linear, Transverse to Flow 52.0 µm/m-°C
28.9 µin/in-°F
z, before Tg; IPC TM-650 2.4.24
Arlon 25N Low-Cost Ceramic Hydrocarbon
High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont..
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
28.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON OE002 PPS - LINEAR
LNP* STAT-KON* OE002 is a compound based on PPS - Linear resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.