Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 59.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 59.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA (Asia Pacific) LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |