Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® GRM2600L ABS High Impact , good chemical resistance sheet grade ABS designed for refrigerator liner applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -20.0 - 150 °C |
40.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC Available in a wide range of colors. Recommended for unpainted exterior/high heat/high impact applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -20.0 - 150 °C |
40.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC (Asia Pacific) Weatherable, injection moldable ASA+PC blend. In a wide range of colors. Recommended for unpainted exterior/high heat applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® BM5225X PC (Asia Pacific) BM5225X resin is a mineral filled grade featuring of high modulus, good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance .. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Asia Pacific) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34XXP PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL-4034 HP is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DI001E PC (Europe-Africa-Middle East) LNP* Lubricomp* DI001E is a compound based on Polycarbonate resin containing Silicone. Added features include: Internally Lubricated, Easy Molding. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC (Europe-Africa-Middle East) LNP* Lubricomp* DL0029E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFL42 PC LNP* Lubricomp* DFL-4042 a compound based on Polycarbonate resin containing 10% Glass Fiber, 20% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp RFL38 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL38 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp UL004AS PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, countaining PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific) 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DX12411C PC LNP* STAT-KON* DX12411C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DX89795 PC (Europe-Africa-Middle East) LNP* STATKON* DX89795 is a compound based on Polycarbone resin containing Carbon Powder. Added features include: Electrically Conductive, Easy Molding, Mold Release. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP 2X98703 ETFE LNP* THERMOCOMP* 2X98703 is a compound based on ETFE Copolymer resin containint Proprietary Filler(s). |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM Test |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM Test |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp PB00A PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PB00A is a compound based on PA 6 resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP QC006I PA 6/10 LNP THERMOCOMPâ„¢ QC006I is a compound based on Nylon 6/10 containing 30% Carbon Fiber. Added features of this grade include: High Impact. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl GTX GTX8110 PPE+PA (Europe-Africa-Middle East) GTX8110 is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaksThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl N1251 PPE+PS ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Asia Pacific) PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Lubricomp XL004 Amorphous Polyamide LNP* Lubricomp* XL-4040 is a compound based on Amorphous Nylon, containing PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Thermocomp® QF-1006 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X5630P PET+PC (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |