Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP COLORCOMP D1000 PC (Europe-Africa-Middle East) LNP* COLORCOMP* D1000 is a compound based on Polycarbonate resin containing Unfilled Custom Color |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DL002 PC (Europe-Africa-Middle East) LNP* Lubricomp* DL002 is a compound based on Polycarbonate resin containing PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Europe-Africa-Middle East) LNP* Lubricomp* DL003 is a compound based on Polycarbonate resin containing PTFE. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRILOY RF206AXH PA 66 LNP LUBRILOY* RF206AXH is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material include: Wear Resistant, Healthcare. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP PFB55 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB55 is a compound based on PA 6 resin containing Glass Bead, Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA6.12 LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX8120P PPE+PA (Europe-Africa-Middle East) GTX8120P is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaks |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3100 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3210 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15 Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT2VZ-15H PA6T/66-GF15 Information provided by EMS Grivory |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 55.0 - 160 °C |
41.7 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide A24G6K PA66, 30% Glass Fiber Reinforced, Heat stabilized, Injection Molding Staramide A24G6K is an Easy Flow, Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG6 PA66, 30% Glass Filled, Injection Molded AG6 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnite® A06 700 PET (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-HGM24 PA410-(GF+MD)30 10% Glass Reinforced, 20% Mineral Reinforced, Heat Stabilized |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LBV-65H FWA black 9225 PA12-GF65 Product description: Grilamid LBV-65H FWA black 9225 is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features High stiffness combined.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RF006XXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006XXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006)Information provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | z, below Tg; IPC TM-650 2.4.24 |
Arlon 45NK Woven Kevlar® Reinforced Laminate and Prepreg 45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic c.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359 |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359 |
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 is an impact-modified, 15% glass fiber reinforced injection molding PA6 grade. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TZ6 280 PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |