Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature -30.0 - 30.0 °C |
77.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
PolyOne Edgetek® X TR2-20TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | Average above Tg, Result based on 450G; ISO 11359 |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 358-10 Cellulose Acetate Propionate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 264-10 CAB Cellulose Acetate Butyrate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP BC 310 EF 600065 Nylon 6 PA 6, injection molding and extrusion grade, non-reinforced, elastomer modified, high impact strength, good flowability (Easy Flow) |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 23.0 - 60.0 °C |
77.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP HAL23 PA11 (Europe-Africa-Middle East) LNP* LUBRICOMP* HAL23 is a compound based on PA 11 resin containing Aramid Fiber, PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature -40.0 - 40.0 °C |
77.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 23.0 - 60.0 °C |
77.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp M10009A PP (Europe-Africa-Middle East) LNP* STARFLAM* M10009A is a compound based on Polypropylene resin, containing Flame Retardant. Added features include : Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® F232-D Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
Covestro Desmopan® DP 3970D Polyurethane, 20% Glass Filled injection molding grade20 % Glass fiber reinforcedgood heat resistancelow coefficent of linear thermal expansionApplicationAutomotive engineeringInjection molded engineering partsPreprocessingMax. W.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K240-HP (Dry) Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EM740 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 16 LM PA12 Product Description: Grilamid L 16 LM is a , low viscosity extrusion type, based on Polyamide 12 (PA12). Grilamid L 16 LM is UV- and heat stabilized. The modification with a nucleation agent results.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 20 GM PA12 Product Description: Grilamid L 20 GM is a medium viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics. Special features of.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 20 LM PA12 Product Description: Grilamid L 20 LM is a medium viscosity Polyamide 12 (PA12) extrusion grade. Grilamid L 20 LM is UV and heat stabilized and has been modified with a nucleation agent which result.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 20H FWA black 9225 PA12 Product Description Grilamid L 20 H FWA black 9225 is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA black 9225 is used for technical injection molded .. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® R 50 H NZ PA6 Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: V.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 3817 black 9992 PA12 Product description: Grilamid XE 3817 black 9992 is a medium viscosity, heat and UV-stabilized Polyamid 12. Grilamid XE 3817 black 9992 is especially suitable for the coating of metal tubes and offe.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 3926 black 9992 PA12 Product description: Grilamid XE 3926 black 9992 is a low viscosity extrusion type, based on Polyamide 12 (PA 12). The special features of Grilamid XE 3926 black 9992 are: Very good chemical resista.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 23.0 - 55.0 °C |
77.8 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6
(Unverified Data**) Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EL630 63 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 20H FWA nat PA12 Product Description: Grilamid L 20 H FWA natural is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA natural is used for technical injection molded parts.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 Z PA12-I Product Description: Grilamid L 25 Z is a UV- and heat stabilized high viscosity polyamide 12 grade with improved toughness. A special feature of Grilamid L25 Z is its high energy absorption capacit.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LKN-3H PA12-GB30 Product description: Grilamid LKN-3H is a 30% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 20.0 - 60.0 °C |
77.8 µin/in-°F @Temperature 68.0 - 140 °F |
TMS2 Perkin Elmer |
Arkema Group Orgalloy® RS 60E10 Polyamide Alloy Polyamide Alloy, Rigid Blown film gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K223-P2 Impact Modified Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EL630 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® F232-DH Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K225-KWS Nylon 6 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25A NZ PA12-I Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid.. |