Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.75 µm/m-°C @Temperature 24.0 - 593 °C |
6.528 µin/in-°F @Temperature 75.2 - 1100 °F |
H900 Condition |
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
CTE, linear | 11.75 µm/m-°C @Temperature 24.0 - 593 °C |
6.528 µin/in-°F @Temperature 75.2 - 1100 °F |
H900 Condition |
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
CTE, linear | 11.75 µm/m-°C @Temperature 24.0 - 593 °C |
6.528 µin/in-°F @Temperature 75.2 - 1100 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
CTE, linear | 11.75 µm/m-°C @Temperature 24.0 - 593 °C |
6.528 µin/in-°F @Temperature 75.2 - 1100 °F |
H900 Condition |
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
CTE, linear | 11.75 µm/m-°C @Temperature 24.0 - 593 °C |
6.528 µin/in-°F @Temperature 75.2 - 1100 °F |
H900 Condition |
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |