Polymer Property : CTE, linear = 18.3 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 33.0 - 44.0 µm/m-°C

@Temperature 0.000 - 20.0 °C
18.3 - 24.4 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
Proto3000 Accura® Bluestone™ Stereolithography (SLA) Prototyping Polymer
Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features:Exceptional stiffnessHigh temperature resistanceExcellent accuracyHigh humidi..
CTE, linear 33.0 - 44.0 µm/m-°C

@Temperature 0.000 - 20.0 °C
18.3 - 24.4 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
3D Systems Accura® Bluestone™ Plastic for SLA® Systems
A high stiffness engineered nanocomposite that opens new applications for stereolithography users. For use with solid-state stereolithography (SLA®) systems.ApplicationsWind-tunnel testing for the ..
CTE, linear 33.0 µm/m-°C

@Temperature 0.000 - 120 °C
18.3 µin/in-°F

@Temperature 32.0 - 248 °F
100 x 15 x 3 mm sample; AZDEL Test
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia..
CTE, linear 33.0 µm/m-°C

@Temperature 0.000 - 120 °C
18.3 µin/in-°F

@Temperature 32.0 - 248 °F
100 x 15 x 3 mm sample; AZDEL Test
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
CTE, linear 33.0 µm/m-°C

@Temperature 0.000 - 120 °C
18.3 µin/in-°F

@Temperature 32.0 - 248 °F
longitudinal direction, 100 x 15 x 3 mm sample; AZDEL Test
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This..
CTE, linear 33.0 µm/m-°C

@Temperature 0.000 - 120 °C
18.3 µin/in-°F

@Temperature 32.0 - 248 °F
100 x 15 x 3 mm sample; AZDEL Test
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
CTE, linear 33.0 µm/m-°C

@Temperature 200 - 300 °C
18.3 µin/in-°F

@Temperature 392 - 572 °F
ASTM TMA
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
U-60 grade Celazole® polybenzimidazole (PBI) resin is a organic polymer which does not burn in air and has high temperature resistance, along with excellent stability to chemicals and hydrolysis. ..