Polymer Property : CTE, linear = 23.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 23.0 µm/m-°C

@Temperature 0.000 - 150 °C
12.8 µin/in-°F

@Temperature 32.0 - 302 °F
Y-Direction; IPC-TM-650 2.1.41
Rogers Corporation Syron™ 7000 Thermoplastic Circuit Material
SYRON™ 7000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7000 is thermally stable, with a ..
CTE, linear 23.0 µm/m-°C

@Temperature 0.000 - 140 °C
12.8 µin/in-°F

@Temperature 32.0 - 284 °F
Z-Direction; ASTM D3386
Rogers Corporation TMM® TMM3 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
CTE, linear 23.0 µm/m-°C

@Temperature 0.000 - 150 °C
12.8 µin/in-°F

@Temperature 32.0 - 302 °F
Y-Direction; IPC-TM-650 2.1.41
Rogers Corporation XT/duroid™ 8000 Thermoplastic Laminate, Circuit Material
XT/duroid™ 8000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 8000 circuit materials ar..
CTE, linear 23.0 µm/m-°C

@Temperature <=100 °C
12.8 µin/in-°F

@Temperature <=212 °F
ISO E 830
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified
Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance..
CTE, linear 23.0 µm/m-°C

@Temperature -30.0 - 0.000 °C
12.8 µin/in-°F

@Temperature -22.0 - 32.0 °F
Alpha 1
Tra-Con Tra-Bond 546S04 Thixotropic UV/Blue Light Cure Adhesive
TRA-BOND 546S04 is a thixotropic UV/blue light curable adhesive with a secondary heat cure. TRA-BOND 546S04 is ideal for general optics bonding, mounting of lenses, and glob top applications. The ..
CTE, linear 23.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.8 µin/in-°F

@Temperature 32.0 - 212 °F
x direction; IPC TM-650 2.4.24
Arlon CuClad 233 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 233 uses a medium fiberglass/PTFE ratio to balance lower dielectric constant and improved dissipation factor without sacrificing mechanical properties.Cross Plied Woven Fiberglass, alternatin..
CTE, linear 23.0 µm/m-°C

@Temperature 25.0 - 150 °C
12.8 µin/in-°F

@Temperature 77.0 - 302 °F
ASTM TMA
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
U-60 grade Celazole® polybenzimidazole (PBI) resin is a organic polymer which does not burn in air and has high temperature resistance, along with excellent stability to chemicals and hydrolysis. ..