Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.1 µm/m-°C @Temperature 25.0 - 250 °C |
9.48 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 4.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 25.0 - 250 °C |
9.48 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 15% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 25.0 - 250 °C |
9.48 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 0% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 25.0 - 250 °C |
9.48 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 10% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 25.0 - 250 °C |
9.48 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 20% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 25.0 - 250 °C |
9.48 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 25% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 25.0 - 250 °C |
9.48 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 30% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |