Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ASTM D648 |
ExxonMobil LL 8455.24 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ASTM D648 |
ExxonMobil LLP8455.24 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 58.7 °C | 138 °F | ASTM D648 |
ExxonMobil HD 6510 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 58.7 °C | 138 °F | ASTM D648 |
ExxonMobil HD 6510.17 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 - 64.0 °C | 138 - 147 °F | Average value: 62.3 °C Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 - 72.0 °C | 138 - 162 °F | ASTM D648 |
DSM Somos® 7110 Epoxy Photopolymer, UV Postcure
(discontinued **) DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ASTM D648 |
ScanTube FEP Tubing Information provided by ScanTube, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ISO 75-2 |
Borealis Borpact™ SG321MO Polypropylene Random Heterophasic Copolymer for Injection Molding Borpact SG321MO is a specially designed modified relatively soft and transparent polypropylene random heterophasic copolymer intended for injection molding. Borpact SG321MO has excellent flow, is f.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | Method A; ASTM D648 |
Formosa Plastics Formolene® HL3812 Film (Hexene) HDPE Medium Density Polyethylene Formolene® HL3812 is a high molecular weight hexene copolymer resin that is tailored specifically for geomembrane applications. The resin provides an excellent balance o.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ISO 75 |
Unitika TERRAMAC TP-4000 Polylactic Acid (PLA) Basic grade, Extrusion, blow, and foam sheet grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | |
Covestro Desmopan® 372 Thermoplastic Polyurethane Desmopan 372 is a TPU on the basis of a special ester.Applications: Transport rolls, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 58.7 °C | 138 °F | ASTM D648-98c |
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 - 61.0 °C | 138 - 142 °F | Thermal Postcure; ASTM D648-98c |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ASTM D648 |
ExxonMobil LL 8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ASTM D648 |
ExxonMobil LL 8555.25 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 58.9 °C | 138 °F | ASTM D648 |
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 58.9 °C | 138 °F | ASTM D648 |
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 58.9 °C | 138 °F | ASTM D648 |
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 58.9 °C | 138 °F | ASTM D648 |
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ASTM D648 |
ExxonMobil LLP8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ASTM D648 |
ExxonMobil LLP8555.25 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ASTM D648 |
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 250 System Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 250 system.Typical ApplicationsMulti-purpose modelsRTV mold patternsForm/Fit/.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ASTM D648 |
ExxonMobil LL 8555.67 Rotational Molding Resin
(discontinued **) LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | |
Covestro Texin® 255 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | ASTM D648 |
DSM Somos® ProtoCast™ AF 19122 Antimony-free Liquid Photopolymer Product DescriptionDSM Somos® ProtoCast™ AF 19122 is an antimony-free liquid photopolymer specifically formulated for producing investment casting patterns.ApplicationsIdeal for use in foundry app.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | |
BASF Novolen® 2900 NC Polypropylene Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | |
BASF Novolen® 3300 MC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | injection molded specimen; ASTM D648 |
Phillips Sumika Marlex® CHP-055 Thermoplastic Polyolefin
(discontinued **) Applications: Passenger-side Air--bag coverSoft interior trimInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product ha.. |